Back to search

Case Western Reserve University School of Graduate Studies

The measurement and origin of fracture toughness in polyethylene

Abstract

dc:description

Fatigue crack propagation studies on annealed and quenched MDPE specimens showed the lifetime of annealed specimens to be one third that of the quenched specimens. The less tortuous crack path of the annealed specimens was traced to a voided and relatively weak annealed root craze, as compared to a continuous tough quenched root craze. DSC and DMS revealed a multiphase annealed morphology but a more homogeneous quenched morphology. The larger quantity of tie molecules was believed to be a major factor in the improved fracture resistance of the quenched specimens. A method to calculate fracture toughness, J 1C, from fatigue tests was developed by utilizing the energy definition of the J integral. In HDPE, it was shown that the new fatigue method yields J 1C values which are nearly identical to those obtained using the standard ASTM bending method. Using the new method, specimen thicknesses, and hence morphologies, can be tested which more closely approximate the thickness of the real component. In addition, the new method permits the calculation of J 1C from brittle fractures of some tough MDPE resins which do not demonstrate brittle fracture with the ASTM method. By varying the loading conditions, different amounts of damag e are produced at the propagating fatigue crack tip. Since the J integral is a measure of the crack tip deformation field, J 1C was observed to vary with loading conditions. A linear relationship between the length of the damage zone and J 1C was observed to be independent of loading conditions, specimen geometry, and material. Since brittle failures in polyethylene generally occur as a result of the material being exposed to low stresses for long periods of time, and since J 1C was not able to distinguish differences in fracture resistance between different MDPEs, a method which utilizes time and energy to calculate the "power to fracture" is introduced. The proposed method yields the same "power band" for one MDPE tested under a variety of conditions and is able to distinguish between different MDPEs. Fatigue crack propagation studies were conducted on two very different specimen geometries. Extensive damage analysis was conducted to determine the types and extent of crack tip damage which developed in both specimens. The summation of these damage types is proportional to the resistance moment, which was employed in the crack layer theory to calculate the specific enthalpy of damage and the dissipation coefficient. Both specimens had the same specific enthalpy of damage, ∼300J/g, and the dissipation coefficients, β SEN=4.6× 10-5, β arc=1.1× 10-4, were inversely proportional to the number of cycles to failure.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Macromolecular Science
Grantor dc:publisher
Case Western Reserve University School of Graduate Studies
Year dc:date
1993

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Strebel, Jeffrey Jerome
Contributors dc:contributor
  • Moet, Abdelsamie

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Strebel, Jeffrey Jerome. The measurement and origin of fracture toughness in polyethylene. doctoral thesis, Case Western Reserve University School of Graduate Studies, 1993. http://rave.ohiolink.edu/etdc/view?acc_num=case1056650936