Back to search

Case Western Reserve University School of Graduate Studies

Dislocations and mechanical properties of single crystal molybdenum silicide

Abstract

dc:description

Dislocations and mechanical properties of single crystal MoSi<sub>2</sub> have been investigated. Specimens were tested in compression along (001), (021), and (771) axes at strain rates of 1 × 10<sup>-4</sup>/s and 1 × 10<sup>-5</sup>/s and at temperatures ranging from 900-1600°C in vacuum or argon. The yield stress along (001) was an order of magnitude greater than that measured along (021) or (771) and along all orientations the yield stress was strongly dependent on temperature. Rate jump tests performed along (001) at 1400°C revealed that the yield stress was rate sensitive with a stress exponent of 4. The activated slip systems were determined using optical slip trace analyses and techniques in transmission electron microscopy. Slip occurred via five different slip systems (11<100>, 13<100>, 1001/2<111>, 131/2<331>, and 111/2<111>) depending on the orientation, temperature and strain rate at which each test was performed. The critical resolved shear stress was determined for the activated slip systems from the measured 0.2% yield stresses. At 900-1100°C, the lo west critical resolved shear stresses were for slip on the 11<100>, 1101/2<111> and 131/2<331> slip systems while at 1200-1600°C the lowest critical resolved shear stresses were for slip on the 11<100> and the 13<100> slip systems. Decompositions and dissociations of 1/2<331> and 1/2<111> dislocations were observed. The 1/2<331> dislocation decomposes into 1/2<111> and <110> dislocations during deformation at temperatures above 900°C. This decomposition prevents deformation by the 1/2<331> dislocation at temperatures of 1200°C and above. HREM observations of the core of a 1/2<331> dislocation revealed that it was dissociated out of the 13 glide plane after deformation at 900°C, while observations of the core of a 1/2<111> dislocation after deformation at 1100°C revealed that it was dissociated by glide in the 110 plane. These core structures strongly affect the Peierls stress for glide of the 1/2<331> and 1/2<111> dislocations. Large climb dissociations of the 1/2<111> and 1/2<331> dislocations were also observed on the (001) plane, possibly resulting from the precipitation of Si vacancies on dislocations. A detailed comparison of these results with those of Umakoshi, Sakagami, Hirano and Yamane (1990) was undertaken by testing material provided by Umakoshi along (001) at 1000, 1300 and 1400°C and along (771) at 1100°C at a strain rate of 1 × 10<sup>-5</sup>/s. Marked differences were observed and explained by the dislocation substructure observed after deformation.

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Materials Science and Engineering
Grantor dc:publisher
Case Western Reserve University School of Graduate Studies
Year dc:date
1994

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Maloy, Stuart Andrew
Contributors dc:contributor
  • Heuer, Arthur

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Maloy, Stuart Andrew. Dislocations and mechanical properties of single crystal molybdenum silicide. doctoral thesis, Case Western Reserve University School of Graduate Studies, 1994. http://rave.ohiolink.edu/etdc/view?acc_num=case1057592461