Abstract
dc:descriptionIn Chapter 1, the hierarchical structure and the failure processes of woven carbon/epoxy composites were studied. The effect of matrix modification on the failure modes was clarified. Reflection and stereo optical microscopy were exploited to investigate the composite structure and to study the composite fracture. Four-point flexure test was used to assess the composite strength. Composite failure was analyzed by monitoring, in-situ, the development of the failure process by using acoustic emission (AE) technique and traveling optical microscopy. Hierarchical structure of the composite was described in three scales; composite, ply, and yarn. Structure imperfections were identified and described. Fracture study proved that the main failure process was delamination and the matrix modification did not influence neither the composite strength nor the failure process. In chapter 2, deformation behavior and damage development of urethane methacrylate resins under tri-axial stress conditions were studied. Type I tensile samples with central hole were cyclically stressed with increasing increment of strain after each cycle until fracture. The strain development at the central hole root, at the top and bottom of each cycle, was monitored using photoelastic technique. Using the color fringes induced by strained polymer at the central hole root, the deformation behavior of the resin was divided into three regions. Region I: linear and recoverable, region II: non-linear and recoverable, and region III: non-linear and non-recoverable. The transition between region I and II occurred at about 2.8% maximum shear strain for all resins. The on-set displacement of damage development, non-recoverable deformation, i.e., transition between region II and III, occurred at different values. These on-set displacements of non-recoverable strains increases as the soft segment content of the resin increased. The fracture surface of the resins resembled those of glass and brittle polymers with their characteristic mirror, mist, and rough regions. The size of the mirror region, the shape of marks on the mist region, and the three-dimensionality of the rough region reflected the pre-fracture damage observed and the soft segment content of the resin.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Macromolecular Science
- Grantor dc:publisher
- Case Western Reserve University School of Graduate Studies
- Year dc:date
- 1994
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Elleithy, Rabeh Hosny
- Contributors dc:contributor
-
- Baer, Eric
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=case1057696304