dc:descriptionTin oxide derived from sol-gel yielded nano-size crystals. Tin oxide (cassiterite) crystals were present in the sol-gel dried at 100° C, and crystallization rapidly increased at 700° C and above. At temperatures below 700° C, the grain growth kinetics showed a weaker time dependence (grain growth exponent n of 6-7.4) with an activation energy of 20-25 kJ/mol, and no growth anisotropy was observed. At 1100° C, n was about 4, consistent with pore control by surface diffusion as a dominant growth mechanism. The results at high temperatures (950 and 1100° C) showed faster growth along the direction normal to (101) than the [110] direction. No significant grain growth was observed for 10-day anneals at 300° C after the material had been calcined at 600 or 800° C. Spin-coating of sol-gel materials provides continuous, porous, polycrystalline thin films with nanometer particle size. Particle and pore size increase with heating temperature and time. The films show (101) texture, and this texture becomes enhanced with increasing heat-treatment temperature. For the same fabrication conditions, films on platinum electrodes exhibited more cracks than those on polycrystalline alumina substrates. Rougher substrates resulted in more cracks. The critical film thickness for cracking on alumina substrate with 970 nm roughness was less than that for alumina with 280 nm roughness. Most of the cracks were located in the valleys between alumina grains. Cracking most likely occurs during drying, but these cracks enlarged and widened during subsequent calcining at 700° C. Doping with Ru suppressed SnO<sub>2</sub> nucleation from the gel materials and slowed down the grain growth (n=8.1-8.9) up to 700° C. Ru doping also reduced the (101) texture of the thin film and the peak intensity relationship returned to the values for SnO<sub>2</sub> powder (i.e. I<sub>101</sub>/I<sub>110</sub> = 0.75) at 800° C. Doping with Pt increased SnO<sub>2</sub> grain size due to heterogeneous nucleation in the initial stage of heating. The grain size difference between Pt-doped and undoped SnO<sub>2</sub> is larger for 1 h heat-treatment than for 24 h heat-treatment at 500-800° C. For heat-treatments from 1 h up to 24 h, Pt doping significantly suppressed SnO<sub>2</sub> grain growth (n=7.6-11.9), resulting in preferential grain growth in the direction normal to (101). Two kinds of surfactants were studied to modify the substrate. Thiol (-SH) surfactant attached only to screen-printed platinum ink via S-Pt bonds, while trichlorosilyl (-SiCl<sub>3</sub>) bonding group surfactant attached to both alumina and platinum ink. The hydrophilic sulfonate-modified surfaces promoted film adherence and resistance to ultrasonic agitation. The hydrophobic methyl-modified Pt surfaces exhibited reduced film adhesion.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Materials Science and Engineering
- Grantor dc:publisher
- Case Western Reserve University School of Graduate Studies
- Year dc:date
- 2004
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Tang, Yin
- Contributors dc:contributor
-
- De Guire, Mark
Subjects
dc:subject × 7Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=case1089995414