Abstract
dc:descriptionThe crystallization of near-eutectic amorphous Ni–P can be significantly retarded by alloying a small fraction of tungsten. Complimentary characterization techniques are applied to understand this phenomenon. DSC (differential scanning calorimetry) reveals the isochronal and isothermalcrystallization kinetics. XPS (X-ray photoelectron spectroscopy) provides core-level electronic signatures of Ni, phosohorus and tungsten, which reflect SRO (short-range order) evolution during crystallization. FEM (fluctuation electron microscopy) provides the MRO (medium-range order)evolution during crystallization. TEM (transmission electron microscopy) provides high-spatial-resolution information on phase nucleation and spatial distribution of atom species. Physical theory has been developed by combining results of these techniques to explain the role of tungsten: Macroscopic aspect (energetics and kinetics), the presence of tungsten reduces the driving force and increases the activation energy for crystallization. Microscopic aspect (micro-mechanistics), the presence of tungsten probably reduces the free volume (hypothesis) due to large atomic radius ratios of rW/rNi and rW/rP; introduces tungsten atoms diffusion to segregate due to chemical potential difference of tungsten in different crystalline phases; involves the breaking of all of W–P bonds with high bond energy. Moreover, theoretical criteria of an effective metal X alloying to improve the thermal stability of M–ML (metal–metalloid) amorphous systems has been proposed. The criteria are: (1) Large negative heat of mixing among X, M and ML. (2) Minimum amorphous free volume by appropriate combination of rX, rM and rML. (3) Large chemical potential difference of X in minor than in major crystalline phase. (4) Large X–ML and X–M bond energy. The criteria conclude on what other potential alloying elements will do, which has implications for fundamental science and technologies. In addition, magnetization curves of as-plated and tempered Ni80P20 and Ni76W4P20 were measured by VSM (vibrating sample magnetometer). Alloying tungsten does not change the paramagnetism of amorphous Ni80P20, but decreases the saturation magnetization ofNi80P20 after crystallization.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Materials Science and Engineering
- Grantor dc:publisher
- Case Western Reserve University School of Graduate Studies
- Year dc:date
- 2017
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Zhan, Xun
- Advisor dc:contributor.advisor
-
- Ernst, Frank
Subjects
dc:subject × 2Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=case1489757814121594