Case Western Reserve University School of Graduate Studies
The Deformation-induced Martensitic Phase Transformation in Low Chromium Iron Nitrides at Cryogenic Temperatures
Abstract
dc:descriptionThe fabrication of the bulk powder a’-phase nitrogen martensite in (Fe<sub>0.99</sub>Cr<sub>0.01</sub>)N<sub>x</sub> system using ball milling at cryogenic temperature was investigated in this thesis. The nitrogen austenite powder particles were sealed in a grinding chamber in a nitrogen atmosphere and ball milled at liquid nitrogen temperature using a cryomill. The amount of martensitic phase transformation was greatly enhanced and the yield of the a’-phase was increased from 28 vol.%, obtained from quench, to 93 vol.% due to the deformation. The X-ray diffractometry and vibrating sample magnetometry measurements were used to determine the martensite phase fraction and the saturation magnetization of the samples. The effect of (1) milling frequency, f, (2) grinding ball size, D, (3) number of grinding balls, (4) total milling time, t<sub>T</sub>, (5) Cr alloying content, and (6) particle size of cryomilled powder on the amount of deformation-induced martensitic phase transformation was studied from a kinetic energy perspective. A model was developed and used to calculate the kinetic energy applied to powder particles during the ball milling process:E<sub>k</sub>=4m<sub>b</sub>·(L-D)<sup>2</sup>·f<sup>3</sup>·t<sub>T</sub>, where m<sub>b</sub> is the mass of the grinding ball and L the length of the grinding chamber. This was correlated to the martensite start temperature with deformation M<sub>d</sub>, M<sub>d</sub> (<sup>o</sup>C)=(68±8)×10<sup>-3</sup>·E<sub>k</sub> (J). The martensite start temperature can then be expressed as M<sub>ST</sub>'=M<sub>ST</sub> [N]+M<sub>d</sub> [E<sub>k</sub>]. The relation between the deformation-induced martensite start temperature M<sub>ST</sub>', which is a function of nitrogen content, and the kinetic energy applied by ball milling was determined to be M<sub>ST</sub>' (<sup>o</sup>C)=(68±8)×10<sup>-3</sup>·E<sub>k</sub> (J)-(169±12) for nitrogen martensite with (10.0±0.1) at.%. nitrogen content. This equation was determined to apply until E<sub>k</sub>=3000J, at which time no further transformation occurred. At 3000J< E<sub>k</sub><10000J, no additional transformation occurred beyond the 93 vol.% maximum. Further increasing the kinetic energy leads to decomposition of the martensite to the equilibrium alpha-phase and gamma prime-phase at E<sub>k</sub>>10000J. The lattice parameters of the gamma-phase as a function of nitrogen content were determined in (Fe<sub>0.99</sub>Cr<sub>0.01</sub>)N<sub>x</sub> system to estimate the nitrogen content in the nitrogen austenite in the samples: a(nm)=0.3604+[(4.6±0.5)×10<sup>-4</sup>]·C<sub>N</sub> (at.%). The saturation magnetization of the a’-phase with (10.0±0.1) at.% nitrogen content was determined to be (233±9) emu/g.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Materials Science and Engineering
- Grantor dc:publisher
- Case Western Reserve University School of Graduate Studies
- Year dc:date
- 2018
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Feng, Zhiyao
- Advisor dc:contributor.advisor
-
- Matthiesen, David
Subjects
dc:subject × 13Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=case1526306156203016