<p>Miniaturization of Nitinol-based medical devices requires increased performance from less material, and therefore necessitates investigation of the connection between material processing and performance. Moreover, it is imperative to understand how impurities that result from processing affect its lifetime performance. Research on the microcleanliness (i.e. presence of nonmetallic inclusions, intermetallic particles, etc.) of fine Nitinol wires and its effect on fatigue performance are not frequently found in literature.</p><p>This study compared a manufacturer-defined standard (SP) and high (HP) purity, Nitinol superelastic (SE) fine (< 140 μm) wire. Nonmetallic inclusion (NMI) chemistry was determined to be Ti<sub>x</sub>Ni<sub>y</sub>O<sub>z</sub> with varied morphology, occurring with/without pores. Combined NMI/pore area percentages ranged from 0.08% ± 0.04% (HP) to 1.44% ± 0.26 (SP) when measured with scanning electron microscopy (SEM). Plasma focused ion beam (PFIB) serial sectioning was also used characterize the combined NMI/pore volume percentages yielding 0.09% (HP) and 0.47% (SP).</p><p>Differential scanning calorimetry was used to identify SE transformation temperatures. Microindentation hardness measurements showed gradients with the center of the wire measuring 359 ± 6.4 HK (HP) and 329 ± 7.2 HK (SP) while mid-radius values were similar for both at 366 ± 5.1 HK and 361 ± 6.0 HK, respectively. Higher tensile and upper plateau strengths were observed in SP (1573 MPa and 515 MPa, respectively) than HP (1420 MPa and 392 MPa, respectively) with greater reduction in area for HP (92.2%) vs. SP (80.2%). Fatigue enhancement was observed in HP wires in flex bending fatigue at strain amplitudes (ε<sub>a</sub>) from 0.67-11% with a run-out at 10<sup>6</sup> cycles and rotating bending fatigue (ε<sub>a</sub>= 1.2-1.5%) though run-out at 10<sup>8</sup> cycles. Fractography showed crack initiation attributed to NMIs/pores at the surface or sub-surface with feature areas ranging from submicron to 20.4 μm<sup>2</sup>.</p><p>Characterization techniques showed that HP contained less large-dimension NMIs/pores than SP leading to less potential stress concentrations and points for crack initiation. These differences in relative purity were reflected in the fatigue results where the HP exhibited enhanced fatigue resistance in both low cycle fatigue and high cycle fatigue regimes.</p>

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Materials Science and Engineering
Grantor dc:publisher
Case Western Reserve University School of Graduate Studies
Year dc:date
2018

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Gbur, Janet L.
Contributors dc:contributor
  • Lewandowski, John

Subjects

dc:subject × 6

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Gbur, Janet L.. Inclusion Effects on the Lifetime Performance of Superelastic Nitinol Wires. doctoral thesis, Case Western Reserve University School of Graduate Studies, 2018. http://rave.ohiolink.edu/etdc/view?acc_num=case153256740897449