Case Western Reserve University School of Graduate Studies
DYNAMIC BEHAVIOR OF COMMERCIAL PURITY POLYCRYSTALLINE MAGNESIUM AT ELEVATED TEMPERATURES AND HIGH STRAIN-RATES
Abstract
dc:descriptionMagnesium and its alloys have become promising materials for applications in the automotive and aerospace industries due to their high specific strength to weight ratios relative to traditional structural metals, such as steel. These materials have been widely investigated in order to improve their mechanical properties, including their ductility, formability, yield anisotropy, elevated temperature performance, to name a few. However, significant questions remain as to how magnesium and its alloys behave under high strain-rate loading and at elevated temperatures. The aim of this dissertation is to develop an understanding of the dynamic plastic response of polycrystalline commercially pure magnesium, including the underlying mechanisms of its deformation under extreme thermo-mechanical loading conditions.In view of this, elevated temperature reverse-geometry normal plate impact experiments as well as combined compression-and-shear plate impact experiments are conducted on polycrystalline commercially pure (99.9%) magnesium using a newly developed elevated-temperature plate-impact experimental configuration. The normal plate impact experiments show a progressive softening in the material’s longitudinal impedance with increasing test temperatures in the range 23 to 500°C. At higher test temperatures from 500 to 610°C, no apparent net change in dynamic stress is observed. However, at still higher test temperatures (617°C and 630°C), a dramatic increase in free surface particle velocity occurs, which indicates anomalous increase in longitudinal impedance of the heated magnesium flyer and the dynamic stress supported by the magnesium in the vicinity of the impact (flyer/target) interface. Microstructural characterization of pre- and post-impact magnesium samples recovered from the normal plate impact experiments reveal an anomalous increase in twin area fraction at temperatures above 610°C. This increase in twinning activity at test temperatures approaching the melt point of magnesium is indicative of increased slip resistance to plastic flow at incipient plasticity at the high strain rates and elevated temperatures approaching melt in pure magnesium. Next, a series of plate impact experiments is conducted using the newly developed elevated temperature combined pressure-and-shear plate impact configuration to investigate dynamic shearing resistance of polycrystalline thin films of pure magnesium. Magnesium foils of two different thicknesses are used – 100 μm thick foils that enable plastic shearing strain rates of ~ 105 s-1, and thinner 25 μm thickness foils that allow plastic shearing rates in excess of 106 s-1 in the samples. In both cases, normal compressive stress in the sample at impact is ~ 4.6 GPa. The measured dynamic shear-stress versus shear-strain profiles show a two-stage deformation response. During Stage I, the sample is observed to deform at relatively low shear stresses, which are observed to increase rapidly with strain at the beginning of Stage II. During this deformation period, the samples are understood to accumulate shear strain by both slip and deformation twinning, simultaneously. Slip is understood to encompass all slip systems with a favorable CRSS, e.g. basal and prismatic slip systems. This relatively low shear stress deformation mode (Stage I) continues until extension twinning is exhausted, resulting in reorientation of the grains in the sample, and shifting deformation to other higher CRSS slip systems and deformation twinning modes including their interactions, in Stage II. It is interesting to note that for the case of thicker foil samples deformed at plastic shear strain rates of ~ 4.8x105s-1, the upturn in shear stress at the transition point (from Stage I to Stage II) occurs at ~ 0.25 shear strain. This transition point shifts to the right as the plastic shear strain rates in the sample are increased -- the transition point increases to 0.32 shear strain at 7.5x105s-1 and to 0.77 as the shear strain rate is increased to 1.45x106s-1 in the 25 μm thick foil samples. Since deformation twinning and dislocation slip are competing mechanisms, twining is expected to be suppressed when the slip activity increases; in other words, the critical twin volume fraction is reached at a higher shear strain, exhibiting a delay in transition from Stage I to Stage II.At room temperature, the shear stress levels during Stage I are observed to plateau at ~170 MPa prior to transitioning to Stage II. Also, while in the higher plastic shear strain rate cases the shear stress is observed to reach the saturation stress almost immediately after impact, in the case of the lowest shear strain rate the shear stress is observed to evolve (harden) over a shear strain of 0.075 before reaching the saturation stress. A striking feature of the deformation in Stage I is the absence of strain hardening even for the two highest plastic shear strain rate cases, which show accumulated plastic shear strains of 0.32 and 0.77, respectively, prior to reaching the transition point. This lack of strain hardening is attributed to the combined effects of geometric strain softening and extension twinning operative during the deformation. The basic idea of geometric softening is that as the sample is deformed (sheared under confined compression-and-shear), a slip system will rotate towards an orientation that is more favorable for slip. This geometric softening along with twinning competes with material strain hardening processes, becoming the dominant effect at larger strains. Another significant result inferred from the elevated temperature combined pressure-and-shear plate-impact experiments is that the shearing resistance of pure polycrystalline magnesium occurs at progressively lower levels of shear stress as the test temperatures are increased from room to 487°C. Contrary to the experiments conducted at room temperature, at elevated temperatures, significant strain hardening is observed in Stage I all the way up to the Stage II transition point. As the shear strain rate is increased, the transition point is again observed to shift to higher levels of shear strain with transition occurring at ~0.9 shear strain at shear strain rate of ~1.45x106 s-1 at 390°C. It is to be noted that the shear stress level (~142MPa) for the 390°C experiment is lower than that obtained at room temperature at nearly the same shear strain rate, but is higher than those measured at higher test temperatures but at lower strain rates. This higher strain and strain-rate hardening in the elevated temperature experiments is understood to be due to the involvement of the higher CRSS slip systems during shearing because of thermal softening, resulting in an increase in overall slip activity when compared to twinning, leading to strain hardening and possibly higher rate sensitivity of the active slip systems.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- EMC - Mechanical Engineering
- Grantor dc:publisher
- Case Western Reserve University School of Graduate Studies
- Year dc:date
- 2019
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Wang, Tianxue
- Advisor dc:contributor.advisor
-
- Prakash, Vikas
Subjects
dc:subject × 3Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=case156233794566219