Case Western Reserve University School of Graduate Studies
INVESTIGATING THE STRUCTURE-PROPERTY RELATIONSHIPS OF POLY(3-ALKYLTHIOPHENE)S AND AZADIPYRROMETHENE-BASED ORGANIC SEMICONDUCTORS
Abstract
dc:descriptionReplacing inorganic semiconductors with organic semiconductors (OSCs) in electronic devices is a promising way to make cheap, light-weight, and flexible electronic devices. Currently, charge carrier mobility of OSCs rivals that of amorphous Si, however, they suffer from mechanical brittleness that limit their application. Simultaneously improving mechanical properties while maintaining charge carrier mobility is challenging since both are orthogonally affected by film morphology, which is affected by the chemical structure. To understand how to optimize both properties it is thus imperative to systematically study chemical structure-property relationship. Regioregular poly(3-alkylthiophene)s (P3AT) are easy to synthesize conjugated polymers (CPs) with good electrical properties, but tend to be brittle, limiting their application. In chapter 2 and 3, we functionalize the side chains of P3ATs to improve their mechanical properties. In chapter 2, we investigate incorporating ester groups in the side chains of poly(3-hexylthiophene) (P3HT) and poly(3-dodecylthiophene) (P3DDT) six carbons away from the polymer backbone. The best combination of robustness and charge carrier mobility is obtained for the P3HT random copolymer with 10\% ester-functionalized side chain: a high fracture strain (296%) combined with a high tensile strength (3.90.6 MPa) resulted in a large toughness (9030 J/m3). This is achieved while maintaining the same high charge carrier mobility as a similar MW P3HT (0.120.01 cm2 V-1 s-1). Side chain modifications do not improve mechanical properties of P3DDT-based copolymers as much, most likely because the longer dodecyl side chains can crystallize, resulting in microphase separation of the side chain and main chain. As a result, side chain modification has little plasticizing effect on the P3DDT main chain for 0-50% ester content copolymers. These results demonstrate that side chain modification with ester-functionality can optimize both mechanical and electrical properties of P3ATs, especially when the side chains and main chain are miscible and behave as one phase.In chapter 3, we synthesize a series of P3HT copolymers with ester- and hydroxyl-functionalized side chains at 5 and 10 mol%. We find that ester and hydroxyl functionalizations at low levels do not affect the optical and thermal properties nor the molecular packing. In terms of mechanical properties, P3HT-5E and P3HT-5H have similar robustness: Elastic's modulus: ~105 MPa, tensile strength: ~6 MPa, fracture strain: ~10%, and toughness: ~ 40 J/m3. At 10% functionalization, the ester-functionalized P3HT is the most deformable; it has the lowest Elastic’s modulus (~90 MPa) and highest tensile strength (~7 MPa), fracture strain (~20 MPa), and toughness (~90 J/m3). On the other hand, hydroxyl-functionalized P3HT is the most brittle; it has the highest Elastic’s modulus at ~140 MPa, but similar tensile strength, fracture strain, and toughness to P3HT copolymers at 5% functionalizations. We conclude that ester groups can soften CPs while hydroxyl groups make the CPs stiffer. In chapter 4, we switch to the development of electron acceptors for organic photovoltaics. We vary the nature (hexyl v hexyloxy) and placement (proximal v distal) of solubilizing groups on a novel series of aza-BODIPY with 2-naphthylethynyl groups on the pyrrolic positions to optimize self-assembly and morphology. Differential scanning calorimetry analysis showed that complexes with hexyloxy solubilizing groups at the proximal and distal positions have stronger intermolecular interactions than those with hexyl solubilizing groups. Cyclic voltammetry analysis results indicated that the electron-donating nature of hexyloxy groups make the BF2(pOhexL2) and BF2(dOhexL2) easier to oxidize than the BF2(phexL2) and BF2(dhexL2). BF2 complexes with distal solubilizing groups have lower HOMO and LUMO levels than those with proximal solubilizing groups. The availability of these complexes with enable future study of the effects of solubilizing groups on film morphology and device properties.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Chemistry
- Grantor dc:publisher
- Case Western Reserve University School of Graduate Studies
- Year dc:date
- 2024
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Tran, Quynh D.
- Contributors dc:contributor
-
- Sauve, Genevieve
- Burda, Clemens
Subjects
dc:subject × 2Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=case1699267477170762