dc:descriptionThis research study investigates the fabrication and mechanical property performance of Stainless Steel 316H (SS316H) processed via two advanced manufacturing techniques: Selective Laser Melting (SLM) Additive Manufacturing and Spark Plasma Sintering (SPS). It also focuses on optimizing the SLM parameter for optimal results. While SS316L has been extensively studied in additive manufacturing (AM) and SPS, limited research exists on SS316H, a high-carbon variant designed for high-temperature applications like Boilers, Turbines, and Nuclear Power Plant Reactors. The research aims to evaluate the influence of processing parameters on densification, microstructural evolution, and mechanical properties, providing a comparative analysis of these two fabrication techniques.SS316H samples were fabricated using SLM at varying volumetric energy densities (VEDs) and SPS at different sintering temperatures, applied pressures, and dwell times. The mechanical performance of the processed samples was assessed through relative density measurements, microhardness testing, tensile testing in both the XY and XZ direction planes, and fracture surface analysis and microstructure analysis via scanning electron microscopy (SEM). Additionally, X-ray diffraction (XRD) and Wear tests were performed to examine the phase composition and tribological properties.Results indicate that SPS-produced samples have superior grain refinement and higher density, leading to enhanced tensile properties compared to SLM samples. However, the SLM-processed samples exhibited higher hardness due to finer microstructural features resulting from rapid solidification. Optimal VED conditions for SLM-processed SS316H were determined to be in the range of 102-107 J/mm³ (with 150 watts of laser power or above), where improved mechanical properties were observed with minimal defects. The SPS samples sintered at 1100°C at 50 MPa for 5 minutes give an impressive tensile result (ultimate tensile strength of 731.20 MPa and strain 77.12%).
Degree
thesis:*- Name thesis:degree_name
- Master of Science in Mechanical Engineering
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Washkewicz College of Engineering
- Grantor dc:publisher
- Cleveland State University
- Year dc:date
- 2025
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Khattab, Mohammad Saif Ali
- Advisor dc:contributor.advisor
-
- Borkar, Tushar
Subjects
dc:subject × 11Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=csu1765802362575733