Abstract

dc:description

<p>Kinetics of iron carbonate and iron sulfide scale formation in CO<sub>2</sub>/H<sub>2</sub>S corrosion was investigated by individually studying iron carbonate formation in pure CO<sub>2</sub>corrosion, iron sulfide formation in N<sub>2</sub>/H<sub>2</sub>S corrosion, and the mixed iron carbonate/sulfide formation in CO<sub>2</sub>/H<sub>2</sub>S corrosion.</p> <p>The first part of the project was to investigate kinetics of iron carbonate scale formation in CO<sub>2</sub> corrosion. A unified iron carbonate solubility expression which accounts for both temperature and ionic strength effects was proposed based on the literature data. The weight change method was developed to more accurately define kinetics of scale formation in CO<sub>2</sub> corrosion and demonstrated that the old data from literature are one to two orders of magnitude too high. Based on the experimental data, a reliable iron carbonate formation equation was developed to describe iron carbonate scale growth on the steel surface in CO<sub>2</sub> corrosion.</p> <p>The second part of the project was to investigate the mechanism and kinetics of iron sulfide formation in N<sub>2</sub>/H<sub>2</sub>S environment. The solubility limits of hydrogen sulfide and iron sulfides were clarified based on the literature data. Using weight change method, both the corrosion rate of the steel and the retention rate of the scale were found. It was also concluded that mackinawite is the predominant iron sulfide formed on the steel surface under the test conditions studied, most likely by a direct reaction of H<sub>2</sub>S with the underlying steel. Based on the experimental results, a mechanistic model of uniform H2S corrosion of mild steel was presented that was able to predict corrosion rate with time.</p> <p>Finally, kinetics experiments conducted in CO<sub>2</sub>/H<sub>2</sub>S solution proved that the makeup of the surface scale not only depends on the water chemistry and the respective solubility of iron carbonate and iron sulfide, but also on the competitiveness of the two scale formation mechanisms. Based on the experimental data it was found that mackinawite was the predominant scale formed on the steel surface which protected the steel from corroding in CO<sub>2</sub>/H<sub>2</sub>S corrosion. The mechanistic model for H<sub>2</sub>S corrosion was extended to predict the CO<sub>2</sub>/H<sub>2</sub>S corrosion process by considering the effect of the presence of CO<sub>2</sub>.</p>

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy (PhD)
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Chemical Engineering (Engineering)
Grantor dc:publisher
Ohio University
Year dc:date
2006

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Sun, Wei
Advisor dc:contributor.advisor
  • Nesic, Srdjan

Subjects

dc:subject × 7

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Sun, Wei. Kinetics of Iron Carbonate and Iron Sulfide Scale Formation in CO<sub>2</sub>/H<sub>2</sub>S Corrosion. doctoral thesis, Ohio University, 2006. http://rave.ohiolink.edu/etdc/view?acc_num=ohiou1163783193