Impact Energy Absorption of Three Mouthguard Materials for Three Environments

Abstract

dc:description

In previous studies at The Ohio State University, significant impact energyabsorption differences were found for mouthguard materials tested in dry and wetconditions. Objective: Measure energy absorption of 3 popular mouthguard materialsexposed to an artificial saliva (Roxane Laboratories, Columbus, OH) and compare toenergy absorption for the dry condition and after conditioning in deionized water.Methods: Thirty specimens with 12.7 cm æmdash; 12.7 cm æmdash; 4 mm dimensions of (a) ethylene vinyl acetate (EVA; T and S Dental and Plastics, Myerstown, PA), (b) Pro-form™ (Dental Resources Inc., Delano, MN), another ethylene vinyl acetate material, and(c) PolyShok™ (Sportsguard Laboratories, Kent, OH), an ethylene vinyl acetatecontaining polyurethane, were prepared following manufacturer recommendations. Tenspecimens of each material were conditioned for 1 h at body temperature (37°C) in thedry condition, deionized water and artificial saliva. Specimens were impacted at 20 mphby a 0.5-inch diameter indenter containing a force transducer (Dynatup Model 9250 HV,Instron Corp., Canton, MA), based upon ASTM (American Society for Testing andMaterials) Standard D3763. Energy absorption was determined from the area under theforce-time curve during the impact event (approximately 5 or 7 millisec depending on thematerial). Groups were compared using ANOVA and the Tukey test. Regions near theimpact site were examined with an SEM. Results: Energy absorption values, normalizedto specimen thickness (mean ± SD in J/mm), were: (a) Dry: EVA (n = 10) 4.73 ± 0.27,Pro-form™ (n = 10) 3.55 ± 0.25, PolyShok™ (n = 10) 6.32 ± 0.24; (b) DI water: EVA (n= 10) 4.82 ± 0.40, Pro-form™ (n = 10) 3.78 ± 0.33, PolyShok™ (n = 10) 5.87 ± 0.38;(c) Artificial saliva: EVA (n = 10) 5.63 ± 0.49, Pro-form™ (n = 10) 4.01 ± 0.54,PolyShok™ (n = 10) 6.37 ± 0.55. PolyShok™ was the most energy-absorbent material inall three environments. EVA was also significantly more impact resistant thanProForm™ in all three environments. EVA and ProForm™ performed significantly betterafter saliva conditioning than dry or water conditioned, but Polyshok™ did not show anydifference in energy absorption when conditioned in any of the three environments.Characteristic deformation patterns from impact loading were observed for each material.Conclusions: The superior energy absorption for PolyShok™ is attributed to thepolyurethane additive.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Dentistry
Grantor dc:publisher
The Ohio State University
Year dc:date
2009

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Lunt, Darin R.
Advisor dc:contributor.advisor
  • Brantley, William

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Lunt, Darin R.. Impact Energy Absorption of Three Mouthguard Materials for Three Environments. masters thesis, The Ohio State University, 2009. http://rave.ohiolink.edu/etdc/view?acc_num=osu1236607924