dc:description<p>The hot-ductility, spot- and longitudinal-Varestraint (mini-Varestraint) tests have long been recognized as useful weldability tests for both quantifying heat-affected zone (HAZ) liquation cracking susceptibility and developing a fundamental understanding of liquation cracking phenomena. However, test results from the spot-Varestraint and hot-ductility tests, interpreted using "conventional" techniques, were inconsistent in predicting the HAZ liquation cracking susceptibility of Incoloys 903 and 909. This discrepancy was attributed to the lack of a physical relationship between weldability test results and the metallurgical response of a material during testing. In the present study, a test methodology characterizing a thermal crack susceptible region (CSR) has been developed based on the properties of a material during welding as obtained from the hot-ductility test and the criteria assumed in the development of liquation cracking theories. This CSR was experimentally verified using the longitudinal- and spot-Varestraint tests performed on A-286 and Type 310 stainless steels. The thermal CSR is material-specific and represents a true quantification of weldability. Metallographic and fractographic examination of test samples revealed that CSR defined a region in the HAZ in which the bulk material exhibits partial melting during welding. The boundary of the CSR is the location at which grain boundaries exhibit partial melting or liquation. The development of this model has (1) provided a quantitative methodology for predicting HAZ liquation cracking susceptibility, (2) elucidated the physical relationship among weldability test results, liquation cracking theories and material properties, (3) clarified the interpretation of test data from the hot-ductility, the spot-and longitudinal-Varestraint tests and (4) confirmed the criteria assumed in the development of liquation cracking theories which state that cracking results from the localized loss of grain boundary ductility due to liquation. This dissertation addresses the theoretical background and experimental procedure in the development of the new methodology. The methods of data interpretation of the three tests and the metallurgical behavior of a material in the CSR are discussed. The utility of conventional methods of data interpretation of the three tests are also critically reviewed.</p>
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Welding Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 1991
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Lin, Wang-En
- Advisor dc:contributor.advisor
-
- Baeslack, William A.
Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1250875709