The Ohio State University
Microstructure Evolution and Material Flow Behavior in Friction-Stir Welded Dissimilar Titanium Alloys
Abstract
dc:description<p>In certain aerospace structures the joining of dissimilar titanium alloys may be necessary. Fusion welding of these alloys together results in the formation of large beta grains and transformed-beta microstructures that can be deleterious to mechanical performance. Friction-stir welding (FSW) was proposed due to the reported microstructural advantages afforded by the process. The purpose of this study was to friction-stir weld dissimilar titanium alloys (Ti-6Al-4V and Timetal 21S, both 1.27 mm in thickness) together and to investigate how macroscopic flow in the stir zone and the resulting weld microstructure affect mechanical properties. </p><p>Welds were produced using a refractory tool with travel speeds from 50 to 100 mm/min and tool rotation speeds of 2000 to 3500 revolutions per minute (RPM). Basketweave and colony alpha and beta phase in the prior-beta grains formed on the Ti-6Al-4V side of the stir zone and near-HAZ. The Timetal 21S region of the stir zone consisted of refined (approximately 18 μm in diameter) metastable-beta grains compared to 30 μm diameter grains in the Timetal 21S base material. Metallurgical mixing between the two alloys resulted in a unique alpha-beta microstructure in the stir zone with high hardness (450 Vicker’s Hardness Number (VHN)). The hardness increase was attributed to a fine distribution of alpha and beta phase. The highest tensile strength (1.1 GPa, 158 ksi) and elongation (8%) for as-welded specimens occurred when lower rotation speeds (3000 RPM) and highest travel speeds (100 mm/min) were used. Placement of the Timetal 21S on the retreating side resulted in the failure of tensile samples in the Timetal 21S base material. If the Ti-6Al-4V was placed on the retreating side, the failure occurred in the SZ/TMAZ region on the Timetal 21S side of the weld.</p><p>Placement of the Ti-6Al-4V alloy on the retreating side increased the amount of metallurgical mixing between the two alloys by 40% compared to when the Timetal 21S was placed on the retreating side. Electron back-scatter diffraction (EBSD) clearly showed the presence of a TMAZ adjacent to the stir zone on the Timetal 21S side of the weld. This was confirmed by the large number of low angle subgrains within the deformed metastable-beta matrix. A series of aging and solution treatment plus aging heat treatments was given to select as-welded samples. The peak hardness for all regions was obtained for the 500°C-8 hour heat treatment, while the 600°C-8 hour heat treatment effectively equalized the hardness values across the entire weld. The heat treatment response of the metallurgically-mixed alpha-beta microstructure was dependent on alpha stabilizer content. </p><p>In terms of material flow, the material directly ahead of the tool shoulder and pin is swept into the stir zone as high-temperature beta phase, so the transport of material in the stir zone during friction-stir welding was, therefore, found to be dependent on the flow stress-dependent viscosity of the alloys. In addition, subgrain formation leads to harder microstructures, so the flow would be hindered in the TMAZ, and subsequently the SZ, upon stirring.</p>
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Welding Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2010
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Gonser, Matthew J.
- Advisor dc:contributor.advisor
-
- Babu, Sudarsanam Suresh
Subjects
dc:subject × 5Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1268138325