Back to search

The Ohio State University

Weldability Evaluation of Naval Steels

Abstract

dc:description

<p>BlastAlloy160 (BA-160) is a high-strength transformation-toughened steel that was developed to meet the material property requirements for blast-resistant Naval applications. The nominal composition of BA-160 is Fe 0.05C 3.65Cu 6.5Ni 1.84Cr 0.1V wt%. Weldability testing techniques were employed to evaluate and quantify the weldability of BA-160 in relation to Naval alloys HY-100, HSLA-100, and HSLA-65.</p><p>Heat-Affected Zone (HAZ) simulations of BA-160 employed phase transformation techniques to identify martensite as the only austenitic transformation product in the HAZ. The HAZ hardness profile was similar for both single-pass Low Heat-Input (LHI) and High Heat-Input (HHI) conditions; slightly higher hardness was observed for the LHI samples. The maximum hardness of 436 HV and minimum hardness of 347 HV were observed in the Inter-Critical HAZ (ICHAZ) and Coarse-Grained HAZ (CGHAZ) regions, respectively. Slight hardness decreases were observed in both the Sub-Critical HAZ (SCHAZ) and Fine-Grained HAZ (FGHAZ) regions when compared to the Base Metal (BM) hardness of 402 HV. The hardness values were in good agreement with measurements from a Gas Tungsten Arc (GTA) spot weld. The observed hardness trend was attributed to lath martensite and Cu precipitation strengthening mechanisms, as quantified by the Electron Backscatter Diffraction (EBSD) and Atom Probe Tomography (APT) techniques, respectively. Cu segregation to a maximum concentration of 20 at% was measured in the CGHAZ. Hardness recovery in a multi-pass CG + SC HAZ sample, similar to that observed during Postweld Heat Treatment (PWHT), was attributed to the re-precipitation of Cu precipitates during the SCHAZ thermal cycle. Single-pass HAZ regions exhibited higher Charpy V-notch impact toughness than the BM at both test temperatures of 20°C and -50°C.</p><p>In hot-ductility tests, BA-160 exhibited a Nil-Ductility Temperature (NDT) of 1419°C, Nil-Strength Temperature (NST) of 1451°C, and Ductility Recovery Temperature (DRT) of 1303°C. The 148°C Liquation Cracking Temperature Range (LCTR) indicated moderate HAZ liquation cracking susceptibility. This finding was attributed to microstructural evidence suggesting a fully austenitic phase transformation sequence at elevated temperatures, compositional enrichment of Cu and Ni along prior austenite grain boundaries in the Partially Melted Zone (PMZ), and good wetting and penetration of liquid films along the austenite grain boundaries. The Naval alloys each exhibited a rapid decrease in on-heating ductility over a narrow temperature range and a LCTR (40°C - 62°C) indicating low susceptibility to HAZ liquation cracking. Their overall behavior was attributed to incipient grain boundary melting from segregation of impurity elements, the suspected formation of delta-ferrite, and liquid discontinuity in the microstructure.</p><p>In both Belgian Welding Institute (BWI) and Simulated Reheat Cracking (SRC) tests, BA-160 demonstrated ductility values above 40 %RA in the 450°C to 700°C temperature range, implying no susceptibility to reheat cracking. HY-100 exhibited appreciable softening and was deemed highly susceptible according to BWI tests at 550°C and 600°C. HSLA-100 was deemed extremely susceptible at 650°C, exhibited by ductility values below 5 %RA. HSLA-65 was deemed susceptible throughout the 550°C to 700°C temperature range. Interrupted cooling tests resulted in significant increases in ductility of the Naval alloys.</p>

Degree

thesis:*
Name thesis:degree_name
Doctor of Philosophy
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Welding Engineering
Grantor dc:publisher
The Ohio State University
Year dc:date
2010

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Caron, Jeremy Leonard
Advisor dc:contributor.advisor
  • Lippold, John

Subjects

dc:subject × 3

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Caron, Jeremy Leonard. Weldability Evaluation of Naval Steels. doctoral thesis, The Ohio State University, 2010. http://rave.ohiolink.edu/etdc/view?acc_num=osu1285050450