Degradation of polymer/substrate interfaces - an attenuated total reflection Fourier transform infrared spectroscopy approach

Abstract

dc:description

Organic coatings are extensively applied to protect metal structures from corrosion related damage. The durability of such polymer coated adhesively bonded joint structures depend upon the stability of the interfaces between the polymer and the substrate it is coated on. It is economically important to have a thorough understanding of how such interfaces react to a variety of aggressive media that are relevant to real life scenarios. In this thesis, attenuated total reflection Fourier transform infrared (ATR-FTIR) spectroscopy has been used to detect changes at the interfaces between poly (vinyl butyral-co-vinyl alcohol-co-vinyl acetate) (PVB) and ZnSe upon exposure to ozone, humidity and UV-B light. Also, the response of PVB-aluminum interfaces to liquid water has been studied and compared with the same for eponol (epoxy resin, diglycidyl ether of bisphenol A)- aluminum interfaces. In the presence of ozone, humidity and UV-B radiation, an increase in carbonyl group intensity was observed at the PVB-ZnSe interface indicating structural degradation of the polymer near the interface. However, such changes were not observed when PVB coated ZnSe samples were exposed to moisture and UV-B light in the absence of ozone showing that ozone is responsible for the observed structural deterioration. Liquid water uptake kinetics for the degraded PVB monitored using ATR-FTIR indicated a degradation of the physical structural organization of the polymer film. Exposure of PVB coated aluminum thin film to de-ionized water showed water incorporation at the interface. There were evidences for polymer swelling, delamination and corrosion of the aluminum film under the polymer layer. On the contrary, delamination/swelling of the polymer was not observed at the eponol-aluminum interface, although water was still found to be incorporated at the interface. Al-O species were also observed to form beneath the polymer layer. A decrease of the C-H intensities was detected at the PVB-aluminum interface during the water uptake of the polymer, whereas an increase of the C-H intensities was observed for the eponol polymer under these conditions. This is assigned to rearrangement of the macromolecular polymer chains upon interaction with water.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Chemistry
Grantor dc:publisher
The Ohio State University
Year dc:date
2010

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Ghosh, Arijit
Contributors dc:contributor
  • Allen, Heather C.

Subjects

dc:subject × 10

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Ghosh, Arijit. Degradation of polymer/substrate interfaces - an attenuated total reflection Fourier transform infrared spectroscopy approach. masters thesis, The Ohio State University, 2010. http://rave.ohiolink.edu/etdc/view?acc_num=osu1291130563