Back to search

The Ohio State University

Energy Dispersive Spectroscopy Characterization of Solute Segregation in Ti-6Al-4V

Abstract

dc:description

Ti-6Al-4V, or Ti-6-4, remains the most widely used titanium alloy in the US market. There remains little or no work investigating the Energy Dispersive Spectroscopy (EDS) characterization of solute segregation in Ti-6-4 as a function of sample geometry. Specifically, there are limited investigations of reduced sample thickness and its effects on measured sample composition. Using a vertically oriented drop furnace, samples of α/β processed, mill anneal Ti-6-4 were held at temperatures of 954°, 899°C, 843°C, and 788°C followed by a water quench. The resulting microstructures contained primary equiaxed alpha (α) and martensitic, prior-β regions. EDS characterization of heat treated samples was conducted for bulk samples in the SEM, electropolished thin foil samples in the TEM, and samples thinned to 250-350nm in the focused ion beam (FIB) that were investigated at 12.5, 15, and 20 keV. Vanadium was the solute of interest for this analysis since it exhibits pronounced segregation between the primary α and prior-β regions, as illustrated by the pseudo-binary β isomorphous phase diagram for Ti-6-4. Generally, bulk SEM and thin foil TEM EDS analyses for vanadium concentration were in good agreement with one another. However, a trend of decreasing aluminum concentration with increasing accelerating voltage was observed in the thinned SEM samples. Conversely, measured vanadium concentration increased with higher accelerating voltages. For the 954°C heat treatment, vanadium concentrations ranged from 0.3 to 0.9 wt.% for the α phase and from 2.7 to 3.1 wt.% in the prior-β regions. The 899°C heat treatment resulted in vanadium concentration ranges from 0.7 to 1.0 wt.% in the α and 4.3 to 4.5 wt.% in the prior-β region. The measured vanadium concentration for the 843°C heat treatment was between 0.7 to 1.3 wt.% for the α phase and from 4.9 to 5.3 wt.% in the prior-β. The 788°C heat treatment resulted in vanadium concentrations of 1.5 to 1.9 wt.% in the α and 8.6 to 9.6 wt.% in the prior-β region.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Materials Science and Engineering
Grantor dc:publisher
The Ohio State University
Year dc:date
2011

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Peterson, Brian
Advisor dc:contributor.advisor
  • Fraser, Hamish

Subjects

dc:subject × 1

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Peterson, Brian. Energy Dispersive Spectroscopy Characterization of Solute Segregation in Ti-6Al-4V. masters thesis, The Ohio State University, 2011. http://rave.ohiolink.edu/etdc/view?acc_num=osu1293718338