dc:description<p>Friction Stir Welding (FSW) was invented by TWI in 1991 and primarily used to join aluminum (Al) alloys. The cost benefit of FSW in Al has led to an increased focus on the use of FSW to join hard metals such as steel, titanium (Ti), and nickel (Ni) based alloys and the materials used to join hard metals. The welding of hard metals creates an extremely high stress region coupled with high temperatures (up to 1300 ¿¿¿¿C in some regions) which promotes tool degradation. Tool degradation and cost of the material are currently the largest challenges to the implantation of FSW of hard metals in industry. </p><p>Previous studies have focused upon investigating alloys suitable to withstand the harsh environment associated with joining hard metal and tool degradation mechanisms. The studies have found that W-based alloys are suitable for joining steel alloys up to 19-mm thick. The studies have also displayed that tools degrade by deformation, abrasive wear, and adhesive wear. Other studies displayed that tool material composition has a large effect of the tool’s susceptibility to tool degradation and degradation mechanisms.</p><p>Previous work has failed to account for the effects of tool microstructure on tool degradation. This study focused upon the effects of tool microstructure on tool material performance. W-Re was selected for this study. Two microstructures were investigated in this study and were an extruded microstructure and a recrystallized microstructure. The investigation was conducted by first performing a short parameter development, followed by a tool life investigation on X-70 steel at identical welding parameters and identical tool designs for each tool material. Subsequent weld passes were ran until a defect was formed, and then the tool was redressed (remachined) to its original profile. The process was repeated until the tool could no longer be redressed. Tool degradation was characterized by pre and post weld microstructure characterization and geometry measurements taken after each weld and redress. The study demonstrated that an extruded microstructure was 27.5% more resistant to tool degradation than the recrystallized microstructure. Both tools lost the majority of the material from the material taper, and primarily by abrasive wear. The recrystallized microstructure also experienced intergranular failure, which may have accelerated the rate of the abrasive wear.</p>
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Welding Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2012
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Michael, Eff
- Advisor dc:contributor.advisor
-
- Babu, Sudarsanam
Subjects
dc:subject × 2Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1332459020