Back to search

The Ohio State University

Comparison of Metal-Ceramic Bond Strengths of Four Noble Alloys using Press-on-Metal (PoM) and Conventional Layering Techniques

Abstract

dc:description

Background: New noble alloys for metal-ceramic restorations being introduced by manufacturers are generally lower-cost alternatives to traditional higher-gold alloys. In order to make a rational alloy selection, knowledge of the values of metal-ceramic bond strength for these alloys is necessary. The evolution of metal-ceramic bond evaluation has changed from a variety of bond strength tests to the adoption of a porcelain adherence test where bond strengths were not evaluated, and then back to the current bond strength test that has been adopted by the American Dental Association as Standard No. 38, which is a modification of International Organization for Standardization (ISO) Standard 9693. With the current dental laboratory protocol for the conventional layering technique, opaque porcelain is first layered on the cast alloy surface following the oxidation step and sintered, followed by layering of body porcelain and perhaps incisal porcelain, which are also sintered; the final glaze may require a separate sintering step, or a self-glazing heating cycle may be used. Ivoclar/Vivadent has introduced new Press-on-Metal (PoM) technology, in which the ceramic is hot-pressed onto the cast metal surface after sintering of the opaque porcelain, and a final glaze step follows after pressing. The objective of this study was to evaluate the bond compatibility index (bond strength) of four recently introduced noble alloys, one high-gold alloy and three more economical alloys, bonded to a compatible porcelain, using the current ISO standard and conventional layering and Press on Method techniques. Methods: Four noble porcelain-fused-to metal alloys: (1) Aquarius Hard, a high-gold alloy (86.1Au-8.5Pt-2.6Pd-1.4In), (2) Evolution Lite, a reduced-gold alloy (40.3Au-39.3Pd-9.3In-9.2Ag-1.8Ga), (3) Callisto 75 Pd, a Pd-Ag-containing alloy (75.2Pd-2.5Au-7.1Ag-9.3Sn-1.0In), and (4) Aries, a conventional Pd-Ag alloy (63.7Pd-26.0Ag-7.0Sn-1.8Ga-1.5In) were selected for bonding to a leucite-containing veneering porcelain (IPS InLine for conventional layering technique and IPS InLine PoM for PoM technique). All products are marketed by Ivoclar Vivadent. Ten metal-ceramic specimens meeting the dimensional requirements for ISO 9693 were prepared for each alloy using recommended manufacturer techniques and the standard porcelain layering and Press-on-Metal methods used in dental laboratories. The three-point bending test in the ISO standard was performed to determine the bond strength. Values for the four alloys were compared using two-way ANOVA (maximum likelihood analysis) and the Tukey test (α = 0.05 for statistical significance).Results: Mean values with standard deviations for bond strength (MPa) using conventional layering were: Aquarius Hard (50.7 ± 5.5; Evolution Lite (40.2 ± 3.3); Callisto 75 Pd (37.2 ± 3.8); Aries (34.0 ± 4.9). For the PoM technique, mean values with standard deviations for bond strength (MPa) were: Aquarius Hard (50.7 ± 5.5; Evolution Lite (40.2 ± 3.3); Callisto 75 Pd (37.2 ± 3.8); Aries (34.0 ± 4.9). From the statistical analyses, the following significant differences were found: (1) The metal-ceramic bond strength for Aquarius Hard was significantly higher for the conventional porcelain layers, compared to the PoM technique. (2) The metal-ceramic bond strength for Aquarius Hard specimens with the conventional porcelain layers was significantly higher than the metal-ceramic bond strengths for the other three alloys with conventional porcelain layers. (3) The metal-ceramic bond strength for the Aquarius Hard specimens with conventional porcelain layers was significantly higher than the metal-ceramic bond strength for (a) the Callisto 75 Pd specimens with conventional porcelain layers and (b) the other three alloys with the PoM technique.Conclusions: For conventional layering and PoM techniques, all four noble alloys had mean metal-ceramic bond strength that substantially exceeded the 25 MPa minimum in the ISO standard. The results for Aries support the manufacturer recommendation not to use the PoM technique for alloys containing over 10% Ag. Clinical selection of these alloys will depend upon other mechanical properties such as yield strength and modulus of elasticity.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Dentistry
Grantor dc:publisher
The Ohio State University
Year dc:date
2012

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Khmaj, Mofida R.ajaili
Advisor dc:contributor.advisor
  • Brantley, William

Subjects

dc:subject × 5

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Khmaj, Mofida R.ajaili. Comparison of Metal-Ceramic Bond Strengths of Four Noble Alloys using Press-on-Metal (PoM) and Conventional Layering Techniques. masters thesis, The Ohio State University, 2012. http://rave.ohiolink.edu/etdc/view?acc_num=osu1338398303