The Ohio State University
Thin films of organic-based magnetic semiconductors for organic spintronics
Abstract
dc:descriptionOrganic-based magnets have been very intriguing and full of opportunities ever since its discovery. Among these materials, V[TCNE]x (TCNE: tetracyanoethylene) has been one of the most studied subjects due to its high magnetic ordering temperature. Its function as spin polarizer has recently been demonstrated that was significant step and promising for the development of organic spintronics. In this thesis, two methods, molecular layer deposition (MLD) and reactive evaporation, for growing thin films of V[TCNE]x are discussed.MLD was introduced to deposit thin film of V[TCNE]x by sequential reactions of V(CO)6 and TCNE. The growth was monitored by a quartz crystal microbalance (QCM). The resulting film has V:TCNE ratio of 1:~0.6 determined by X-ray photoelectron spectroscopy (XPS). It has RMS roughness ~0.5 nm for a 30 nm-thick film. The coercive field was ~80 Oe at 300 K and magnetic-order temperature up to 400 K, which indicates the MLD-made material is a harder magnet with enhanced thermal stability with respect to the CVD-made V[TCNE]x. The activation energy was determined to be 0.45 eV and has been utilized in both organic/inorganic hybrid and all-organic spin-valve devices. To further broaden the coverage of this material, the MLD of thin films of Co-TCNE and Co-V-TCNE have also been demonstrated.A deposition system was designed and built for the PVD-based reactive evaporation. Thin film V[TCNE]x was synthesized by depositing V under partial pressure of TCNE. The resulting film showed low RMS roughness (~0.2 nm). The coercivities varied with temperature ranges from 60 to 80 Oe, and the magnetic order temperature was higher than 400 K. The composition of the resulting films could be tuned by varying the V flux as well as the TCNE partial pressure. The V:TCNE ratios were determined both by QCM and XPS. The coercivity and magnetic behavior did not show significant change upon the variation of V:TCNE ratio within the range of 0.5-1. This method is advantageous not only in its simplicity and potentially broad choice of metal elements, but also in its compatibility of using shadow mask for device fabrication.
Degree
thesis:*- Name thesis:degree_name
- Doctor of Philosophy
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Chemistry
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2012
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Kao, Chi-Yueh
- Contributors dc:contributor
-
- Epstein, Arthur
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1343748166