The Ohio State University
Study of Corrosion and Corrosion Inhibition of Chromate and Chromate-Free Primers
Abstract
dc:description<p>Chromate and chromate-free primers were characterized in this study. For chromate primer examined, PPG EWEDA 144A (Pittsburgh Plate Glass Company), SrCrO4 was the active inhibitor. The three chromate-free primers examined were Deft 02GN084, Hentzen 16708 TEP and Sicopoxy 577-630. In the Deft product, the active inhibitor was PrO/ Pr(OH)3. CaSiO3 was the active inhibitor for Hentzen 16708 TEP and BaSO4 for Sicopoxy 577-630. How each pigment reacted within its coating environment during exposure was an object of study and primers coatings were characterized by several techniques. Focused ion beam (FIB) milling was used to prepare cross sections for energy dispersive x-ray analysis (EDX) to identify pigments and inhibitors derived from them. A MatlabTM program was developed to analyze the resulting EDX maps to characterize the dispersion of elements in inhibitor ions produced by pigment dissolution during exposure. Pigment characteristics and pigment dissolution varied widely from primer to primer. Chromate pigments were present in high volume fractions in chromated primers. As a result pigment particles were in close proximity to one other and touching in 2D sections. In the chromate-free primers, inhibitor pigment particles were present in much lower volume fractions and were far away from each other.</p><p>To quantify the protectiveness of chromate and chromate-free coatings systems in standard exposure testing on mixed metal structures, optical profilometry was used on painted and primed 7075-T6 coupons outfitted with AISI 316 or Ti-6Al-4V bolts. The presence of the bolts provided galvanic stimulation to corrosion attack occurring under the coating during ASTM B117 exposure. In these experiments, coatings were stripped and corrosion damage was quantified by optical profilometry, which allowed measurement of the total corroded volume that accumulated around the bolts that were placed in the coated samples. The volume was converted to corrosion rate. In general, 316 CRES fasteners caused more serious corrosion to AA2024-T3 panel than Ti-6Al-4V. And samples with chromium-containing pretreatments, Surtec 650 or Alodine 1200S, had smaller corrosion volume that those with adhesion promoter, Prekote or BoeGel. In the aspect of primers, ANAC P2100P003 and Deft 44-GN-098 gave the substrate best protection, while PPG EWDE 144A and Henzten 17176 KEP had the worst performance on corrosion prevention among the six types of primers examined. In addition, the application of topcoat did not guarantee a better protection on the scribed AA2024-T3 panel. And the rate of pigment dissolution was affected by the application of topcoat.</p>
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Materials Science and Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2012
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Li, Longfei
- Contributors dc:contributor
-
- Buchheit, Rudolph
Subjects
dc:subject × 6Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1344896405