The Ohio State University
Fiber Laser Welding of 304 Stainless Steel and the Effects of Various Parameters on Materials Coupling and Back-Reflection
Abstract
dc:description<p>Los Alamos National Laboratory purchased a new 6000 watt IPG fiber laser. During testing of the system, it was discovered that a significant amount of back-reflection was being seen during the ramp-up and ramp-down of power while trying to transition into and out of keyhole mode welding. An investigation was started by looking into the damage mechanisms of a fiber laser. Fiber lasers are susceptible to damage caused by back-reflection at several points within the system. The delivery fiber can be damaged at the cladding boundary by the interactions with impurities at the boundary as well as the active fiber. The pump diodes are not designed to handle any significant amount of 1070 µm wavelength light and can be damaged by it. </p><p>The fibers are damaged due to thermal effects. The glasses and plastics used in construction of the fiber do not conduct heat very well and it can build up quickly causing local vaporization at cladding boundaries or cracking of the fiber. Because of this the laser manufacturers go to extreme lengths to remove back-reflection in their systems. </p><p>This work was conducted in three stages. The first stage was to characterize the focused beam. This was accomplished using the Primes Power Monitor and Primes Focus Monitor. Spot size and focus position shift was determined during this phase. Stage two was to characterize the response of the Beam-switch Scattered Light Detector (BSSLD). Baseline response data was obtained during this phase. </p><p>The final stage was to produce welds and examine back-reflection response and transition to keyhole mode welding. The effects of travel speed, spot size, surface finish, head tilt, shielding gas, plume suppression, and ramping (ramp up or ramp down) were investigated.</p><p>Tilting the head off to the side or away from direction of travel proved to be the most effective method. Titling the head towards the direction of travel produced significant back-reflection. Changing the travel speed, shielding gas, machining the surface, doubling the spot size, and coating the surface had little effect on the amount of back-reflection produced. Both ramp up welds and ramp down welds showed similar back-reflection spikes. A common trait was seen during ramp up weld trials, with the exception of using He gas, there was a point that the back-reflection went to background and then the weld would transition to keyhole mode. This point would occur at powers greater than 300W. A similar point occurred on the ramp down welds. The weld would drop out of keyhole and back-reflection would drop to background and then back-reflection would start to increase. This increase would also start to occur at a little less than the 300W point.</p><p>Starting and stopping the weld at the 300W threshold provided the means to transition between conduction mode and keyhole mode without the risk of producing the excessive back-reflection spike that lead to a laser power increase. This proved to be a viable method to reduce the back-reflection to a safe level in cases where titling the head is just not practical.</p>
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Welding Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2012
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Stellwag, William L., Jr
- Advisor dc:contributor.advisor
-
- Farson, David
Subjects
dc:subject × 4Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1348253254