The Ohio State University
Development of a Coating Formulation Procedure for Ni-base Shielded Metal Arc Electrodes with Varying Core Wire Composition
Abstract
dc:descriptionIn order for manufacturers of shielded metal arc welding (SMAW) electrodes to stay competitive, they must be able to have flexibility in the performance of their products, as well as flexibility in the manufacturing process. Nickel base welding consumables often require specialized chemical compositions which are more stringent than the requirements for the base material on which they are welded. To complicate this problem further, the core wire chemistry often has a target which is a different chemical composition, and different manufacturers may not have the same target composition. To compensate for these variances, alloying elements are often added through the flux coating to adjust the weld deposit composition. Understanding how these additions to the flux coating will affect the weld deposit is critical to the manufacturing process. This work examines two common types of nickel base SMAW electrodes, ENiCrMo-4 and ENiMo-10. Both were manufactured with a baseline coating which did not contain any alloying elements. Then using the same heat of core wire and flux formulation, electrodes were manufactured with multiple iterations of that coating with a single additional alloying element. The electrodes were then welded using a specially designed mechanized SMAW machine. The mechanized SMAW repeated each weld bead as closely as possible in order to minimize any variation in arc length, which may interfere with evaluation of the results. The effects of the various coatings were evaluated to prove the addition’s effectiveness. The tests used in this work are the cast pin tear test, SS DTA measurements, and tensile testing. The effects of each coating addition on all of the alloying element’s recovery rates were compared to find that addition’s overall impact on the weld deposit. The solidification range was measured using single sensor DTA to evaluate the effect of the altered weld metal composition on the solidification range. This was then compared to the solidification range predicted by modeling software. The cracking susceptibility of the altered weld metal was also evaluated using the cast pin tear test. This work demonstrates the first step in creating a logical, methodical process for the determination of the amount of the addition of the alloying elements to the weld deposit through the flux coating. Alloying through the flux allows the manufacturer to compensate for core wires of varying chemical composition. This work also outlined tests which are necessary to verify that the alloying additions did not compromise the integrity of the welding electrode.
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Welding Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2012
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Gaal, Brian
- Advisor dc:contributor.advisor
-
- Lippold, John
Subjects
dc:subject × 2Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1354481846