Back to search

The Ohio State University

Atmospheric Pitting Corrosion of AA7075-T6 Under Evaporating Droplets

Abstract

dc:description

Pitting corrosion of polished and etched AA7075-T6 in the presence of 3.5 wt % NaCl electrolyte was investigated both with standard full immersion testing, and with the application of evaporating electrolyte droplets in a fixed humidity environment. Testing included the addition of chromate-, vanadate, and cerous-based corrosion inhibiting salts in concentrations of 3 mM, 0.3 mM and 0.03 mM. A Scanning Kelvin Probe (SKP) was used to investigate the <i>in situ</i> corrosion potential behavior of the electrolyte droplets.In immersion testing, widespread pitting at intermetallic particles was observed in uninhibited solution. Similar but less severe attack was observed with additions of 0.03 mM vanadate and cerous ions. At higher concentration of vanadate, small numbers of very large pits were found, while higher concentrations of cerous ions provided very good inhibition. Chromate provided nearly complete inhibition of corrosion in all concentrations of immersion testing. In all cases of immersion testing, the measured corrosion potential was found to be pinned near to the pitting potential.In droplet testing, corrosion potentials measured by SKP were indicative of a range of behaviors, including metastable pitting, inhibition/passivation, and a form of corrosion attack in which pitting at the edge of the test droplet resulted in the formation of an adjacent, secondary droplet. This secondary droplet effect, observed in uninhibited NaCl droplets as well as with 0.03 mM concentration of both vanadate and cerous ions, was investigated in more detail with SKP. The attack progresses by large-scale separation of anodic and cathodic regions under the droplet, with the anodic region initiating near the edge of the droplet. A model is described for the formation of the secondary droplet and associated attack, by deliquescence of water vapor due to an excess of ions from the anode diffusing to the edge of the droplet.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Materials Science and Engineering
Grantor dc:publisher
The Ohio State University
Year dc:date
2013

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Morton, Sean C.
Contributors dc:contributor
  • Frankel, Gerald

Subjects

dc:subject × 6

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Morton, Sean C.. Atmospheric Pitting Corrosion of AA7075-T6 Under Evaporating Droplets. masters thesis, The Ohio State University, 2013. http://rave.ohiolink.edu/etdc/view?acc_num=osu1367585533