TIG Welding of Nickel Titanium to 304 Stainless Steel

Abstract

dc:description

Nickel-titanium is a shape memory alloy capable of producing high stresses with an 8% maximum recoverable strain. The rotation of a nickel-titanium (NiTi) torque tube can be controlled by thermally cycling the material through its critical martensite and austenite temperatures. Transforming the phase of NiTi corresponds to a change in its crystalline structure and a macroscopic change in shape. This change in shape, through a controlled thermal input, lends itself well to powering a solid-state actuator. Shape memory alloys can in some cases replace traditional actuators, for instance in harsh aerospace environments where lightweight operation is critical.NiTi is effective as a solid-state actuator, but it is very difficult to machine. The poor machinability of NiTi drives the cost and complexity of system integration to the point where its widespread use is hindered. The general solution is to join NiTi to a structural material and machine the structural material for system integration. Several types of joining methods have been studied such as ultrasonic soldering, adhesives, and laser welding. This study focuses on tungsten inert gas (TIG) welded joints between 304 stainless steel and NiTi tubing. A nickel filler is used in TIG welding of NiTi to 304SS to prevent brittle intermetallics formed by titanium and iron in the weld pool. The thickness of the nickel filler and the current required to create a strong TIG weld in torsion failure is investigated in a Taguchi L9 full factorial test matrix. Based on ultimate failure torque test results and welding observations, a 0.050'' filler thickness with an 85 A starting current was chosen for thermocycling tests with a constant load. The chosen joint parameters produce an average ultimate failure torque of 371 in-lb (41.9 N-m) with a shear strength of 41 ksi (282 MPa). EDS analysis of 0.025'' and 0.075'' filler thickness welds confirm observations from welding and test data with a crack caused by TiFe intermetallics in the 0.025'' filler weld and minimal weld penetration on the 304SS interface with the 0.075'' filler thickness. Results from dye penetrant tests, ultimate failure test data, and sectioned weld analysis were used to gain understanding of TIG welding NiTi to 304SS.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Mechanical Engineering
Grantor dc:publisher
The Ohio State University
Year dc:date
2014

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Riggs, Mark R.
Contributors dc:contributor
  • Dapino, Marcelo

Subjects

dc:subject × 15

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: some rights reserved. It is licensed for use under a Creative Commons license. Specific terms and permissions are available from this document's record in the OhioLINK ETD Center.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

Riggs, Mark R.. TIG Welding of Nickel Titanium to 304 Stainless Steel. masters thesis, The Ohio State University, 2014. http://rave.ohiolink.edu/etdc/view?acc_num=osu1397607979