Analysis of the Degradation and Performance of a Non-Chromate Organic Coating System on AA2024-T3 Using Electrochemical and High-Resolution Microscopy Techniques
Abstract
dc:descriptionThis research investigated the corrosion of a coated metal system through the application of novel sample preparation and high-resolution microscopy techniques. An aluminum alloy 2024-T3 (Al-4.4Cu-1.5Mg-0.6Mn, solution heat-treated, cold-worked and naturally aged) substrate with a SurTec 650 trivalent chromium (Cr) process (TCP) conversion coating, a Deft 02GN084 praseodymium (Pr)-based primer qualified to MIL-PRF-23377 Type I Class N, no top coat and a machine-engraved scribe was prepared at NAVAIR. Preliminary electrochemical impedance spectroscopy experiments were completed to determine water uptake properties of the coating system and analyzed using electrical equivalent circuit models. Subsequently, the sample was exposed in ASTM B117 neutral salt-spray until there was a visible blister under the coating, which took 13 days. Thin foil samples of the substrate/coating interface were prepared using focused ion beam microscopy from exposed locations: (1) inside the scribe, (2) at the end of the blister, (3) near the end of the blister and (4) away from the blister. In addition, a thin foil sample was prepared from (5) an unexposed sample away from the scribe of the same sample type. High-resolution imaging and chemical analysis were performed on each thin foil using scanning transmission electron microscopy and energy dispersive spectroscopy at 300 kV. Thickness maps of each foil were created using low-loss electron energy-loss spectroscopy to locate areas of similar foil thickness for accurate standardless chemical comparisons between samples.It was concluded that water uptake of this coating system occurred in the first 5 hours of full immersion in 0.5 M NaCl, with the onset of corrosion occurring after approximately 70 hours. A method to extract thin foils of substrate/coating interfaces was demonstrated. Furthermore, high-resolution imaging of a substrate/TCP interface was performed for the first time under a coating. There were no detectable inhibitors (Pr and Cr) in the scribe after a 13-day exposure in ASTM B117. Magnesium appeared enriched on the substrate surface and in the TCP region of exposed and unexposed samples, likely an artifact of the coating preparation process. Additionally, deeper chloride ingress ensued with less distance from a blister. Finally, there was no detectable corrosion under an intact coating after exposure, with the caveat that each thin foil represented an extremely localized interfacial region.
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Materials Science and Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2014
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Holguin, Kerrie Nikaido
- Advisor dc:contributor.advisor
-
- Frankel, Gerald
Subjects
dc:subject × 9Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1408732642