The Ohio State University
Processing, mechanical properties, and thermal stability of nickel-aluminide multilayered thin films
Abstract
dc:description<p>Multilayered thin films have been proven to show enhanced properties over bulk materials and conventional thin films. The hardness of multilayers has received much recent attention, as several mechanisms have been proposed to understand the genesis of the improved hardness. In this work, two sets of three films were deposited by DC magnetron sputtering. The samples consisted of alternating layers of Ni-10%Al and Ni3Al; one set had layer repeat distance (¿) of 300 nm and the other set had ¿=50 nm. Within each set, the volume fraction of the constituents was varied between 60% Ni(Al), 50% Ni(Al), and 40% Ni(Al). The films were characterized by X-Ray diffraction, nanoindentation, and SEM in the as-deposited and post-annealed states.</p><p>It was found that as-deposited films all have similar hardness and stress state, but those containing a 60% Ni3Al had a slightly lower stress state and higher hardness than equal-volume fraction films or those containing 40% Ni3Al, regardless of ¿. Following annealing at 673 K, all of the layers retained their structural continuity and experienced an increase in stress state and hardness. Evidence of interface curvature was seen in the 60% Ni3Al films, while the 40% Ni3Al films had flatter interfaces. The ¿=50 nm films exhibited a doubling of hardness, while the ¿=300 nm films increased in hardness by ~25%. The amount of misfit dislocation content at the interfaces does not govern the strength of the multilayered film because thinner bilayers have fewer misfit dislocations but higher hardness.</p><p>Following annealing at 1073 K, the 40% Ni3Al film had profuse grain boundary grooving and many discontinuous Ni3Al layers, while the 60% Ni3Al film had grain boundary grooving that rarely perforated the Ni3Al layers. Both films had interface curvature consistent with grain boundary grooving, but the needle-like aspect ratio of the 60% Ni3Al films provides more resistance to perforation from grooving than the pancake-¬like aspect ratio of the 40% Ni3Al films. Both of the films annealed at 1073 K had much lower stress state and hardness than in the as-deposited condition due to creep processes such as grain-boundary diffusion. The 40% Ni3Al film that exhibited profuse grooving and perforation had a large amount of scatter in the mechanical properties, indicative of an inhomogeneous structure, while the 60% Ni3Al film had consistent mechanical properties.</p><p>It was found that equal-volume fraction ¿=240 nm films annealed at 1373 K and allowed to furnace cool formed a Ni(Al) solid solution at ~100 K below the phase diagram prediction, while ¿=40 nm films annealed at 1273 K and furnace cooled dissolved the Ni3Al layer ~200 K below the solvus line. This is consistent with modeling that the dissolution temperature decreases with decreasing layer thickness. The solutionized structure can be frozen in place by air-cooling of the film.</p>
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Materials Science and Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2003
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Sperling, Evan Andrew
- Advisor dc:contributor.advisor
-
- Anderson, Peter
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1409231969