Welding with Low Alloy Steel Filler Metal of X65 Pipes Internally Clad with Alloy 625: Application in Pre-Salt Oil Extraction
Abstract
dc:descriptionIn the oil & gas industry, extraction of oil reserves from pre-salt subsea oil fields requires pipelines and risers to be joined with welds that overmatch the X65 pipe yield strength by 100 MPa, have high toughness, and do not utilize a PWHT. In typical oil extraction, these internally clad pipes are welded with fill passes of Alloy 625 that match the internal clad, however, the strength requirement for reeling is not met with this alloy. To meet the strength requirement, low alloy steel consumables were studied as fill passes to join X65 pipes that are internally clad with Alloy 625 with root passes welded using 625 filler metal. The problem with this metallurgical combination is that solidification cracking can occur in the low alloy steel weld passes that have been diluted by Alloy 625. Computational modeling was performed to screen potential consumables and welding trails were completed for consumables that demonstrated compatibility. Upon establishing welding parameters, bead-on-plate design of experiments were performed with low alloy steel (ER100S-G) welded over two different nickel-based alloys (Alloy 625 and Alloy 686). Buffer layer solutions were also tested using two other Ni-based alloys, UTP A 80 Ni and Alloy 625 LNb, to isolate the root pass material from the fill pass material. Solidification cracking was eliminated in bead-on-plate welds of ER100S-G over Alloy 625 using small weave amplitudes, however, Alloy 686 was determined to have better compatibility with the low alloy steel filler metal to avoid solidification cracking. Welding experiments in a narrow groove were performed for the compatible combination, ER100S-G fill passes over a root pass of Alloy 686, and solidification cracking was eliminated from the fill pass welds. During this study, a defect previously thought to occur only in castings has been identified in welds of low alloy steel filler metals over Ni-based alloy substrates. Referred to in this study as “shrinkage porosity”, these defects were encountered in the compositional transition zone of these welds and were related to the large difference in solidification temperature ranges between the low alloy steel filler metal and the Ni-base alloy substrate.
Degree
thesis:*- Name thesis:degree_name
- Master of Science
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Welding Engineering
- Grantor dc:publisher
- The Ohio State University
- Year dc:date
- 2016
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- O'Brien, Evan Daniel
- Advisor dc:contributor.advisor
-
- Alexandrov, Boian
Subjects
dc:subject × 11Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=osu1469018389