Back to search

The Ohio State University

Comparison of Load-to-Fracture Values and Fracture Characterization of Monolithic Zirconia, Lithium Disilicate, and Zirconia-Reinforced Lithium Silicate Glass-Ceramic CAD/CAM Crowns

Abstract

dc:description

All-ceramic monolithic crowns have been extensively used in prosthodontics in recent years for their excellent advantages compared to traditional metal-based restorations. In the oral environment, ceramic restorations are susceptible to cyclic fatigue failure, mainly due to the presence of cyclic masticatory forces together with the moist environment. The purpose of the study was to compare the integrity of zirconia, lithium disilicate, and zirconia-reinforced lithium silicate monolithic CAD/CAM crowns after being subjected to cyclic loading in a wet condition and then subjected to static loading until fracture. A fiberglass master die replica was used to fabricate (1) zirconia (Zirkonzahn, South Tyrol, Italy), (2) lithium disilicate (LDS, IPS e.max® CAD, Ivoclar Vivadent AG, Schaan / Liechtenstein), and (3) zirconia-reinforced lithium silicate glass ceramic (ZLS), Vita suprinity, VITA Zahnfabrik, Bad Sackingen, Germany) monolithic crowns that were milled using CAD/CAM technology. The crowns were bonded according to manufacturer instructions and subjected to cyclic loading (10,000 and 50,000 cycles) under wet conditions. Representative specimens from each group were examined using SEM. Analysis of the recorded load-to-fracture values was carried out with two-way (ANOVA) followed by the Tukey-Kramer post hoc test (a=.05). The mean of load-to-fracture values measured were 3232.27 N for 10,000-cycle LDS, 3510.62 N for 50,000-cycle LDS, 1207.69 N for 10,000-cycle ZLS, 761.20 N for 50,000-cycle ZLS, 4967.29 N for 10,000-cycle zirconia, and 5041.99 N for 50,000-cycle zirconia. All mean load-to-fracture values were statistically significantly different (p< .05). However, there was no statistical influence of the number of cycles on the load-to-fracture of test crowns (p > .05). Load-to-fracture values of Zirconia and LDS CAD/CAM crowns were above the reported clinical posterior occlusal forces (720 N according to Gibbs et al.) and ZLS load-to-fracture values were closest to the average posterior occlusal force value. Further clinical and laboratory investigation are needed on the use of ZLS ceramic.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Dentistry
Grantor dc:publisher
The Ohio State University
Year dc:date
2016

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Kashkari, Afnan
Advisor dc:contributor.advisor
  • Yilmaz, Burak

Subjects

dc:subject × 2

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Kashkari, Afnan. Comparison of Load-to-Fracture Values and Fracture Characterization of Monolithic Zirconia, Lithium Disilicate, and Zirconia-Reinforced Lithium Silicate Glass-Ceramic CAD/CAM Crowns. masters thesis, The Ohio State University, 2016. http://rave.ohiolink.edu/etdc/view?acc_num=osu1469039766