Evaluation of the Effect of Tungsten and Boron Additions on the Microstructure and Solidification Cracking Susceptibility of Fe-Mn-C Filler Metals

Abstract

dc:description

High manganese steels are potential candidates for use in cryogenic applications as they exhibit desirable low temperature properties and are a cost-effective alternative to high-Ni steels (i.e. 9%Ni steel, Type 304L) and Invar alloys. Their cryogenic properties are derived from the austenite stabilizing ability of manganese. A potential use for these steels is in the fabrication of liquefied natural gas (LNG) storage tanks. The demand for natural gas is expected to increase 65% by the year 2040 and thus the need for cost-effective materials to replace conventionally used high-Ni alloys during construction of storage and transportation tanks is relevant. When fabricating these LNG tanks, welding is a critical procedure and thus the weldability of these high manganese steels must be evaluated. In this study, the effect of tungsten (W) and boron (B) additions on the microstructure and solidification cracking susceptibility of Fe-Mn-C filler metals was evaluated. Five compositions with tungsten additions up to 4.7 wt% and boron additions up to 27 ppm have been evaluated. Susceptibility to solidification cracking of these filler metals was determined using the Cast Pin Tear Test (CPTT). Solidification simulations were conducted using the Scheil approximation within Thermo-Calc™ and actual solidification temperature range measurements were conducted using the Single-Sensor Differential Thermal Analysis (SS-DTA™) technique. Metallurgical characterization was carried out using both optical microscopy, and scanning electron microscopy. The objective of this study was to determine the optimum range of tungsten and boron additions within the compositional range of interest that provides adequate resistance to weld solidification cracking.Results from Scheil simulations indicated only slight variations in the solidification temperature range (STR) among the alloys tested. The simulations showed that W additions lowered the liquidus temperature and subsequently the STR while B expanded the STR, which is attributed to its strong partitioning effect. Using SS DTA, the measured STR for each composition was larger than the Scheil simulations but demonstrated similar trends. Boron appeared to have the most influential effect on the expansion of the STR in these alloys due to segregation.To assess the solidification cracking susceptibility, two rounds of CPT testing were performed to verify the lower cracking threshold (LCT) and rank the alloys. Both rounds of CPTT results ranked the Base composition (no W or B) as the least susceptible to cracking while the Low W/High B alloy exhibited the highest susceptibility to solidification cracking. A trend from CPTT results showed that higher W additions to both low and high B compositions resulted in a slight increase in resistance to solidification cracking susceptibility. All compositions had LCT values below 1.0 in., indicating that these alloys would be susceptible to solidification cracking, based on previously tested Ni-base alloys using the CPTT. Thus, additions of W to the low B alloys resulted in an increase in cracking resistance.Characterization of CPTT and button samples showed that each filler metal composition exhibited primary austenite solidification with no evidence of martensite (a’ or e) or other primary phases. The CPTT specimens exhibited fracture surface morphologies that were characteristic of solidification cracking. Three secondary phases were identified: Titanium nitrides, manganese sulfides, and titanium sulfides/carbosulfides. No boron rich constituents were found during this investigation and more advanced characterization techniques would be needed to evaluate the segregation behavior of boron. There was no evidence of backfilling in any of the CPTT samples examined that could potentially lead to crack healing. The formation of titanium sulfide/carbosulfide during solidification expanded the solidification temperature range and contributed to the overall poor resistance to solidification cracking exhibited in these alloys. In general, it was determined that the Fe-Mn-C filler metals investigated in this study would be susceptible to solidification cracking under moderate restraint conditions. The presence of boron and sulfur, even at relatively low levels (= 50ppm), promoted an increase in solidification cracking susceptibility. No combination of W and B additions was able to provide adequate resistance to weld solidification cracking. Boron appeared to have the most dominant effect on cracking susceptibility while tungsten had a minor positive contribution. This conclusion was reached based on the findings from the CPTT results, solidification analysis, and metallurgical characterization of these filler metals.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Welding Engineering
Grantor dc:publisher
The Ohio State University
Year dc:date
2016

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Lenzo, Jansen C., Lenzo
Advisor dc:contributor.advisor
  • Lippold, John

Subjects

dc:subject × 14

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Lenzo, Jansen C., Lenzo. Evaluation of the Effect of Tungsten and Boron Additions on the Microstructure and Solidification Cracking Susceptibility of Fe-Mn-C Filler Metals. masters thesis, The Ohio State University, 2016. http://rave.ohiolink.edu/etdc/view?acc_num=osu1470829433