Back to search

The Ohio State University

<i>In-situ</i> scanning tunneling microscopy studies of the SEI formation on graphite anodes in propylene carbonate

Abstract

dc:description

Since its discovery in 1979, the solid electrolyte interface (SEI) has drawn attention due to its importance for efficient battery performance. Despite its significance, there is still some ambiguity with regards to how certain electrolytes form a protective interface to aid Li<sup>+</sup> intercalation whilst others irreversibly degrade the anode structure. One of the most debated examples is the “EC-PC disparity” towards the graphite anode, where ethylene carbonate (EC) results in protective SEI formation whilst propylene carbonate (PC) leads to destructive graphite exfoliation. This study focuses on the correlation between the concentration of the Li<sup>+</sup> salt, LiPF<sub>6</sub> dissolved in PC and the growth of SEI on graphite.<i>In-situ</i> and <i>in-operando</i> electrochemical scanning tunneling microscope (STM) observation of the basal plane of highly oriented pyrolytic graphite (HOPG) is performed in 1 M, 2.5 M and 3 M LiPF<sub>6</sub> dissolved in propylene carbonate (PC) in sequence to cyclic voltammetry (CV) and potential hold experiments. This technique allows the study of the topographic evolution of the basal plane and edge sites on HOPG with changes in the potential, as a result of solvent co-intercalation, reduction, graphite exfoliation and SEI formation. STM images obtained whilst holding the potential at selected values, gives an insight into the nature of SEI formation, in connection to the extent of regeneration of the graphite surface. It is found that below 0.9 V vs Li, solvent decomposition, followed by extensive graphite exfoliation takes place in the 1 M and to a lesser degree in 2.5 M LiPF<sub>6</sub> electrolyte solutions. However, in the 3 M salt solution, graphite exfoliation is scarce and SEI formation is observed at potentials as high as 1.1 V vs Li, which clearly indicates a concentration dependent SEI formation on graphite. CV experiments conducted in parallel to EC-STM, provide further confirmation. The HOPG is cycled between 3 to 0.005 V vs Li in all three salt concentrations within Swagelok® type cells. A comparison of the initial cycle for the three concentrations reveals a shift in the onset potential for solvent reduction towards higher values, specifically, 1.2, 1.4 and 2.0 V for 1 M, 2.5 M and 3 M LiPF<sub>6</sub> in PC. Previous studies have attributed the difference in SEI formation to the competition between the fluoride-containing anion and solvent towards the solvation of Li<sup>+</sup>.

Degree

thesis:*
Name thesis:degree_name
Master of Science
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Chemistry
Grantor dc:publisher
The Ohio State University
Year dc:date
2019

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Dehiwala Liyanage, Chamathka H.
Advisor dc:contributor.advisor
  • Co, Anne

Subjects

dc:subject × 10

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Dehiwala Liyanage, Chamathka H.. <i>In-situ</i> scanning tunneling microscopy studies of the SEI formation on graphite anodes in propylene carbonate. masters thesis, The Ohio State University, 2019. http://rave.ohiolink.edu/etdc/view?acc_num=osu1574502965210263