Back to search

University of Cincinnati

SCRATCH BEHAVIOR OF POLY(carbonate) FILM/SUBSTRATE SYSTEMS

Abstract

dc:description

The effect of adhesion, film thickness and substrate hardness on the scratch behavior of PC film/substrate systems was investigated. Scratch tests were performed using a custom-built scratch tester. The resulting scratches were observed by optical microscopy, atomic force microscopy (AFM), and environmental scanning electron microscopy (ESEM). The critical normal load for delamination/debonding was used as a criterion to determine the scratch resistance of the films. Better film/substrate adhesion or higher film thickness resulted in higher critical loads. The scratch response of PC films depended strongly on the hardness of the substrates on which the films were deposited. Substrates having relatively low hardness (i.e., Al 1100) were severely deformed under the scratching conditions. Intermediate hardness substrates (i.e., Al 6022, Al 6111, and ferroplate) were more resistant to the imposed load; hence, the deformation of the substrates was less severe. High hardness substrates (i.e., glass) resisted the applied load and resulted in higher stress concentration at the interface. Consequently, little or no deformation of these substrates was observed during scratching of PC films on glass substrates. Influence of γ-aminopropyltriethoxysilane (γ-APS) on the scratch behavior of PC films was determined. The critical load of PC films increased rapidly as the concentration of the solutions used to deposit the γ-APS films increased from 0.0 to 0.2 %; thereafter, the critical load increased only slightly as concentration of the γ-APS solutions increased from 0.2 to 5 %. Reflection-absorption infrared spectroscopy (RAIR) and X-ray photoelectron spectroscopy (XPS) were used to examine the chemical reaction at γ-APS/PC interface using diphenyl carbonate (DPC) model compound. RAIR results revealed the formation of urethane and urea linkages between γ-APS and DPC. Curve fitting of high resolution C <sub>1s</sub> spectra showed that the main reaction product between DPC and 0.2% γ-APS was urethanes. Heat treatment of 0.2% γ-APS films resulted in lower critical loads due to higher crosslink structure of the primer. Therefore, diffusion of PC into γ-APS primer was limited. High reaction temperature for γ-APS and PC caused oxidation of amine, however, it increased the probability of amine to react to carbonate due to increasing mobility of PC chains.

Degree

thesis:*
Name thesis:degree_name
PhD
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Engineering : Materials Science
Grantor dc:publisher
University of Cincinnati
Year dc:date
2005

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • WIRASATE, SUPA
Contributors dc:contributor
  • Boerio, Dr. F.

Subjects

dc:subject × 7

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
citation

WIRASATE, SUPA. SCRATCH BEHAVIOR OF POLY(carbonate) FILM/SUBSTRATE SYSTEMS. doctoral thesis, University of Cincinnati, 2005. http://rave.ohiolink.edu/etdc/view?acc_num=ucin1131995339