dc:description<p>High-temperature electronics and MEMS (Micro-Electro-Mechanical Systems) based on polycrystalline diamond (PCD) are promising because of its wide band gap, high thermal conductivity, and large carrier mobility. To take advantage of this opportunity, research was undertaken to develop techniques for the synthesis of both undoped and doped high quality PCD films with good surface flatness suitable for the fabrication of high temperature electronics and MEMS devices. One way to fabricate smooth films is to decrease the grain size because diamond films with large grain size bring forth problems in contact formation and device fabrication due to the large surface roughness. Consequently, there is a need to fabricate nanocrystalline films with small grain size and good smoothness. In addition, the electrical properties and conduction mechanisms in nanocrystalline diamond (NCD) films have not been sufficiently analyzed. This study also aims at achieving high resistivity nanocrystalline diamond films and to study the electrical conduction mechanism.</p> <p>Several approaches have been used in our research to achieve these goals. Initially microcrystalline diamond (MCD) films were grown on silicon (100) substrates by the microwave plasma enhanced chemical vapor deposition (MPCVD) method using methane in a hydrogen plasma environment. Introduction of small amounts of argon into the Argon / Hydrogen plasma was used to deposit diamond films with a range of microstructures from microcrystalline to nanocrystalline grains. A detailed quantitative study of the sp<sup>3</sup>, sp<sup>2</sup> content in the films grown with varying amounts of argon in the plasma was done using Raman spectroscopy. The optimum gas composition that gave the best quality diamond film consisting of 1.6 µm grains was 60% Ar/ 39% H<sub>2</sub>/ 1% CH<sub>4</sub>. The optimum gas composition that gave nanocrystalline grains of size in the order of <50 nm was 95% Ar/ 4% H<sub>2</sub>/ 1% CH<sub>4</sub>. A change in the cross-sectional microstructure from the columnar to grain-like (equiaxed) morphology was observed. The change was attributed to different plasma chemistry with the C<sub>2</sub> dimer as the primary growth species in the Ar-rich plasma. Varying concentrations of N<sub>2</sub> gas were also used to decrease the grain size of the diamond films. The growth species in this case was C<sub>2</sub> at low nitrogen content and CN at high nitrogen content. This can also be used to dope the films n-type, when added in small quantities in order to increase the conductivity of the PCD. Small quantities of nitrogen (<0.1%) gave ultrananocrystalline diamond (UNCD) of grain size less than 10 nm. For N<sub>2</sub> concentrations between 0.1% and 2% diamond films of grain sizes in the range of 100-200 nm were obtained. The addition of boron in small concentrations was used to dope the films p-type. These were useful in making electronic devices.</p> <p>Electrical properties of the microcrystalline and nanocrystalline diamond films were measured over a range of temperatures by fabricating capacitors using a metal-insulator-metal (MIM) configuration that could withstand temperatures up to 600 °C. Typical electrical resistivities of MCD were ∼10<sup>12</sup> Ω.cm while the dielectric constant was near 5.6, which was representative of natural diamond. For NCD, the electrical resistivities were of ∼10<sup>11</sup> Ω.cm was obtained, which was eight orders of magnitude higher than values reported by other researchers. A lower dielectric constant of 5.2 was obtained for the NCD. The electrical conduction mechanisms in undoped MCD, NCD, and nitrogen-doped films were studied. The Hill’s conduction mechanism was dominant in MCD and NCD films due to the deep-level traps present, which contributed to grain-boundary conduction. The average distances between the trap sites were found to be 11 nm for the MCD, and 5 nm for the NCD were estimated. These related to the hopping conduction across impurities present in the grain boundaries. These impurities were attributed to graphite in the PCD films. The nitrogen-doped diamond films were processed to fabricate a metal-insulator-semiconductor (MIS) structure. The resistivity of a 1% nitrogen-doped diamond was 2.8x10<sup>7</sup> Ω.cm. The space-charge-limited-conduction mechanism was suggested for the nitrogen-doped diamond films due to holes injected from the p-type silicon into the n-type diamond layer, and the injected holes played a role of the current carriers.</p>
Degree
thesis:*- Name thesis:degree_name
- PhD
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Engineering : Materials Science
- Grantor dc:publisher
- University of Cincinnati
- Year dc:date
- 2006
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Ramamurti, Rahul
- Advisor dc:contributor.advisor
-
- Singh, Dr. Raj
Subjects
dc:subject × 12Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=ucin1145630189