University of Cincinnati
Electro-Mechanical Behavior of Strontium Modified Lead Zirconate Titanate Ceramics
Abstract
dc:description<p>Since the discovery of perovskite ferroelectrics, the solid solution of PbZrO<sub>3</sub>-PbTiO<sub>3</sub> (PZT) system is intensively studied due to its excellent electro-mechanical properties for transducers and actuators applications. The strontium modified PZT (PSZT) at the Zr rich end shows a long antiferroelectric-ferroelectric boundary suitable for field induced phase transition study and associated electro-mechanical behavior study.</p><p>A modified oxide route was developed to process PSZT ceramics with different Zr<sup>4+</sup>/Ti<sup>4+</sup> ratios for repeatable ultra-high strain applications. Repeatable ultrahigh strain of ~ 0.8% was achieved for PSZT compositions near the A<sub>T</sub>-F<sub>R</sub> phase boundary. Other compositions showed strain (0.35-0.8%) which were still better than the commercially available materials of same class. The PSZT ceramics showed high polarization response as well. Polarization over 41µC/cm<sup>2</sup> was observed for certain ceramics on the F<sub>R</sub> side.</p><p>A novel dynamic in-situ X-Ray diffraction was conducted on the different PSZT ceramics to understand the field induced electromechanical property changes. The ultrahigh strain in these materials, on the antiferroelectric tetragonal side of the phase diagram, was found to be due to unit cell volume change along with the movement of the non 180° domains. For the rhombohedral ferroelectric materials the strain was mostly contributed by the unit cell volume increase. Compositions farther away from the boundary in the AF<sub>T</sub> side did not show any structural change or domain movements.</p><p>Electrical fatigue behavior of PSZT ceramics was investigated by subjecting the as-sintered ceramics to low frequency (30 Hz) electric field up to 10<sup>7</sup> cycles. The fatigue free polarization behavior (<10% degradation) was attributed to the high density and low porosity of the PSZT ceramics. The high strain degradation nature (~50% degradation) was found to be partially due to internal stress development during the electrical cycles and partially due to the formation of fatigue induced mechanical damage layer under the electrode. Thermal annealing and removal of the damaged layer showed the complete recovery of the strain to its original as-sintered value. Some preliminary electric fatigue experiments with electron beam deposited aluminum (Al) electrode were conducted on PSZT ceramics. The results showed promising fatigue resistance behaviors.</p>
Degree
thesis:*- Name thesis:degree_name
- PhD
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Engineering : Materials Science
- Grantor dc:publisher
- University of Cincinnati
- Year dc:date
- 2007
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Dutta, Indrajit
- Advisor dc:contributor.advisor
-
- Singh, Raj
Subjects
dc:subject × 1Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=ucin1187036967