Back to search

University of Cincinnati

Structural Evaluation of LIC-310-0396 Box Beams with Advanced Strand Deterioration

Abstract

dc:description

<p>Four adjacent prestressed concrete box beams were removed from a decommissioned bridge and tested to destruction. The beams were 36 inches wide by 17 inches deep and had a span length of 37 feet 6 inches. Each beam contained fourteen, 1/2 inch diameter, stress relieved prestressed strands. All of the prestressed strands were arranged in one layer, which was located below the stirrups. One beam was in good condition, with the only visible deterioration being longitudinal cracking. One beam had three corroded prestressed strands visible and a large spalled segment which, when removed, exposed two additional prestressed strands. The remaining two beams were badly deteriorated, with spalled concrete exposing seven corroded prestressed strands.</p><p>The provisions of the AASHTO LRFD Bridge Design Specifications, the AASHTO Standard Specifications, and the PCI Design Handbook were used to evaluate the loss of prestressing force. The measured prestressing force loss was closest to the AASHTO LRFD Bridge Design Specifications, but all three methods provided conservative estimates of prestressing force loss.</p><p>The bridge had been designed using the AASHTO Standard Specifications. The provisions of the Standard Specifications were conservative in determining the ultimate loading for the undeteriorated beam. The provisions of the Standard Specifications were also conservative in determining the ultimate load for the deteriorated beam if the deteriorated strands were assumed ineffective. The deteriorated concrete box beams were all ductile and had final deflections exceeding L/50.</p><p>The original bridge was rated using the test results. When following the provisions of the AASHTO Standard Specifications, the designed service loading for the bridge would have exceeded the ultimate loading of one deteriorated middle span beam. A failure of this beam would not have caused a progressive failure of the middle span under service loadings. Following the Load Factor Rating method for the middle span beams, the loadings exceeded the strength of the members. Therefore, load restrictions would have been required for the bridge had it not been decommissioned.</p>

Degree

thesis:*
Name thesis:degree_name
MS
Level thesis:degree_level
masters
Discipline thesis:degree_discipline
Engineering : Civil Engineering
Grantor dc:publisher
University of Cincinnati
Year dc:date
2010

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Lab, Scott
Chair dc:contributor.committeechair
  • Miller, Richard

Subjects

dc:subject × 6

Rights

dc:rights
Statement dc:rights
  • unrestricted
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Lab, Scott. Structural Evaluation of LIC-310-0396 Box Beams with Advanced Strand Deterioration. masters thesis, University of Cincinnati, 2010. http://rave.ohiolink.edu/etdc/view?acc_num=ucin1275657735