University of Cincinnati
Assessment of Pretreatment Strategies to Slow Sensitization Rates in Aluminum Alloy 5083-H116
Abstract
dc:descriptionAluminum alloy AA5083-H116 is widely used in marine, transportation, and structuralapplications, but its susceptibility to sensitization can lead to intergranular corrosion (IGC) andstress corrosion cracking (SCC). Recent results have shown that introducing small amounts ofinitial sensitization at temperatures above 100°C leads to slower subsequent sensitization kineticsin these alloys. Building upon those findings, this study aims to optimize pre-service processingby investigating the effect of pretreatments introducing pre-sensitization levels of 0.5%, 1%, and2% at 160°C, 180°C, and 200°C on the long-term sensitization behavior and mechanical properties.AA5083-H116 samples were heated at each temperature to achieve different pre-sensitizationlevels before being aged at 100°C to assess long-term Degree of Sensitization (DoS) evolution.Tensile tests were conducted to evaluate the effect of sensitization on mechanical properties. Theresults indicate that higher pretreatment temperatures (e.g. 200°C) significantly reduce DoS,confirming that pretreatment suppresses the sensitization kinetics. Additionally, pre-sensitizationlevels of 2% provided comparable corrosion resistance to the previously studied 5% level,suggesting an opportunity to optimize processing. Tensile testing revealed that all heat treatmentsled to a slight reduction in yield strength due to recovery, but ultimate tensile strengths (UTS) risehigher after sensitization due to strain-hardening effects. 160°C pretreated samples retained thebest mechanical integrity, while 200°C pretreated samples experienced greater strength loss,indicating a trade-off between corrosion resistance and mechanical performance, though allconditions remained within standard specifications for the materials.These findings provide an efficient approach to improving corrosion resistance in AA5083-H116,offering potential benefits for industries that rely on wrought aluminum structures, though futureresearch using environmental exposure testing and exploring SCC will be necessary for validation.
Degree
thesis:*- Name thesis:degree_name
- MS
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Engineering and Applied Science: Materials Science
- Grantor dc:publisher
- University of Cincinnati
- Year dc:date
- 2025
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Jayade, Gajanan
- Chair dc:contributor.committeechair
-
- Steiner, Matthew
Subjects
dc:subject × 7Rights
dc:rights- Statement dc:rights
-
- unrestricted
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English