University of Cincinnati
SEMI-CONTINUOUS PLASMA POLYMERIZATION OF A FILM TO ENHANCE THE TEXTURE PROPERTIES OF AN ELASTOMER
Abstract
dc:descriptionThe texture of a styrene butadiene rubber (SBR) film was enhanced by the deposition of a plasma-polymerized, siloxane-like coating. This improvement in texture was quantified as a reduction in the coefficient of friction of the SBR film, from approximately 1.2 for the uncoated material to 0.3 for the coated material. The adhesional forces in the elastomer that result in SBR film having a high coefficient of friction were masked upon the application of the coating. However, the desirable bulk properties of the elastomer such as the extensibility and modulus were retained. A dual-mode reactor, in which both low frequency (LF) and microwave (MW) power were applied to the plasma, was used to yield a deposition rate of approximately 280 nm min-1. During deposition, carrier gases (Ar and O2) were flowed through the reactor, along with the monomer (hexamethyldisiloxane, HMDSO). Batch depositions were performed to determine the reactor parameters that yielded the maximum deposition rate and the minimum coefficient of friction. Semi-continuous depositions were also performed by inserting an unwind and rewind mechanism into the reactor to produce a moving web that simulated an industrial coating process. The molecular structure of the deposited films was determined using attenuated total reflectance (ATR) infrared spectroscopy and found to consist of mainly Si-O-Si and Si-CH3 groups. The thicknesses of the films, and hence the deposition rates, were determined by variable angle spectroscopic ellipsometry (VASE). The coefficient of friction values for the films were determined by tribometry. A film thickness of approximately 100 nm usually resulted in a reduction in coefficient of friction of the SBR material to approximately 0.30. The SBR film was extremely sensitive to increases in the temperature of the LF electrode, due to the applied LF power. However, when the LF power was reduced to 15 W and the MW power was increased to 500 W, the SBR film was processed for a semi-continuous deposition lasting approximately 15 min. Approximately 10 ft of coated material with a low coefficient of friction were produced prior to the web failing due to heating. For the continuous processing of SBR film, the heating of the LF electrode must be controlled.
Degree
thesis:*- Name thesis:degree_name
- MS
- Level thesis:degree_level
- masters
- Discipline thesis:degree_discipline
- Engineering : Materials Science
- Grantor dc:publisher
- University of Cincinnati
- Year dc:date
- 2000
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- CHASE, JENNIFER E.
- Advisor dc:contributor.advisor
-
- Boerio, F. James
Subjects
dc:subject × 3Rights
dc:rights- Statement dc:rights
-
- restricted--full text not available online
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=ucin975349091