Processing Effects on Core-Shell Grain Formation in ZrO<sub>2</sub> Modified BaTiO<sub>3</sub> Ceramics

Abstract

dc:description

Formation of core-shell grains in BaTiO<sub>3</sub> based dielectric ceramics is essential to achieve stable dielectric temperature characteristic. This grain core-shell structure consists of a grain core, which is high purity BaTiO<sub>3</sub>, ferroelectric, and a paraelectric grain shell, where there is a concentration gradient of dopant. Most commonly core-shell additives are ZrO<sub>2</sub>, CeO<sub>2</sub> , Nb<sub>2</sub>O<sub>5</sub> +Co<sub>2</sub>O<sub>3</sub>. As a result, internal stress is generated due to this dopant inhomogeneity within the grain and the normally sharp phase transition at Curie point becomes diffused. Up to now understanding and control of core-shell grains in BaTiO<sub>3</sub> ceramics is still far from satisfying, which is the basis of this thesis work. In this work, processing influences on core-shell grain formation were investigated in the terms of powder size, stoichiometry, particle surface modification by slurry pH and leached Ba<sup>2+</sup>, pressing pressure and additive effects such as ZrO<sub>2</sub> , Nd<sub>2</sub>O<sub>3</sub>, BaO and flux CuO, BaCuO<sub>2</sub>, followed by multiple regression analysis to identify significant variables so as to form core-shell grains in a controller manner. It is found that ZrO<sub>2</sub> amount; powder size, stoichiometry and temperature/time are most significant in control of core-shell characteristic (low Δε%<30%). The desired core-shell characteristic was obtained with the maximum internal stress, which was achieved by the fine and uniform grains along with maximum amount ZrO<sub>2</sub> solid solution in the BaTiO<sub>3</sub> lattice and Ba<sub>2</sub> (Ti,Zr)<sub>5</sub>O<sub>12</sub> ~Ba<sub>2</sub> (Ti, Zr)<sub>9</sub> O<sub>20</sub> second phase developed in the grain shell region; the desirable shell/grain thickness ratio was estimated to ~0.05. Any variation in processing, which favors such structural and micro structural development, facilitates the core-shell formation. It is found that, Ba/Ti surface stoichiometry of 0.5~0.6 facilitated core-shell characteristic, and this chemistry of BaTiO<sub>3</sub> particle surface and optimum additive dispersion can be achieved by neutral slurry pH; With adequate eutectic liquid phase, uniformly distributed fine grain morphology was achieved with high sintered densities. A dielectric formulation of 0.8~1.3 wt% ZrO<sub>2</sub>, and 3 m/o BaCuO<sub>2</sub> and 0.1~0.3 m/o Nd<sub>2</sub>O<sub>3</sub> was successfully developed to be sintered at 1055~1085°C/45~90 min with Δε%<25%. This formulation has the potential to be co-fired with base metal electrodes.

Degree

thesis:*
Name thesis:degree_name
PhD
Level thesis:degree_level
doctoral
Discipline thesis:degree_discipline
Engineering : Materials Science
Grantor dc:publisher
University of Cincinnati
Year dc:date
2001

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Zhou, Lei
Advisor dc:contributor.advisor
  • Buchanan, Relva

Subjects

dc:subject × 6

Rights

dc:rights
Statement dc:rights
  • restricted--full text not available online
  • This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
Language dc:language
English

Identifiers

dc:identifier.*

Chain of custody

source
Harvested from
OhioLINK
Base URL
etd.ohiolink.edu/acprod/odb_etd/ws/oai/oai
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Zhou, Lei. Processing Effects on Core-Shell Grain Formation in ZrO<sub>2</sub> Modified BaTiO<sub>3</sub> Ceramics. doctoral thesis, University of Cincinnati, 2001. http://rave.ohiolink.edu/etdc/view?acc_num=ucin983977793