University of Cincinnati
KINETICS, PROCESSING, AND PROPERTIES OF Si/SiC COMPOSITES FABRICATED BY REACTIVE-MELT INFILTRATION
Abstract
dc:descriptionThe kinetics and mechanism of reaction of carbon with Si melt or Si+Mo melt were investigated. The growth of the reaction-formed SiC layer was found to follow a fourth power rate law. A kinetics model was developed, in which an internal electric field was assumed to be set up over the SiC layer through a negative space charge. The diffusion of carbon-ion vacancies was considered as the rate-limiting step for the growth of SiC layers. The effect of processing temperature and addition of Mo on the kinetics was also studied. Based on the kinetics study, a processing model was developed to relate the Si content in the Si/SiC composites with the porosity in the preforms for the reactive-melt infiltration processes. The minimum porosity was obtained for fabricating completely-reacted, near-net-shape, and fully dense materials. Using this model as guideline, the preforms consisting of α-SiC powder and graphite were designed and made by tape casting followed by hot lamination and binder burnout. The porous preforms were then infiltrated by liquid Si at 1450°C to produce the Si/SiC composites containing 10 to 45 vol.% Si. The composition of the composites were verified by quantitative analyses using X-ray diffraction and image analysis. The effects of Si content on the mechanical properties as well as creep behavior were studied using four-point bending tests. The elastic modulus and flexural strength were reduced with increasing Si content. The change in elastic modulus with Si content followed the rule of mixtures at room temperature. The elevated-temperature flexural strength decreased significantly when Si content was above 20 vol.%. The creep rate increased with Si content, especially when Si content was above 20 vol.%. Composites containing less than 20 vol.% Si exhibited a significant creep resistance up to 1550°C. The stress and temperature thresholds for creep were found for the composites containing more than 20 vol.% Si. Temperature or stress beyond their corresponding threshold value caused a significant acceleration in creep. The creep data were analyzed to identify the creep mechanisms.
Degree
thesis:*- Name thesis:degree_name
- PhD
- Level thesis:degree_level
- doctoral
- Discipline thesis:degree_discipline
- Engineering : Materials Science
- Grantor dc:publisher
- University of Cincinnati
- Year dc:date
- 2001
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- ZHOU, HONG
- Contributors dc:contributor
-
- Singh, Dr. Raj
Subjects
dc:subject × 6Rights
dc:rights- Statement dc:rights
-
- restricted--full text not available online
- This thesis or dissertation is protected by copyright: all rights reserved. It may not be copied or redistributed beyond the terms of applicable copyright laws.
- Language dc:language
- English
Identifiers
dc:identifier.*- Repository record dc:identifier
- http://rave.ohiolink.edu/etdc/view?acc_num=ucin994941745