Back to search

Pohang University of Science and Technology

용액에서 결정화된 전구체를 이용한 폴리에틸렌 옥사이드 나노 패턴의 박막 제조

Abstract

Poly(ethylene oxide) (PEO) films with uniform nanopatterns were prepared by spin-coating aged dilute solutions containing crystallized precursors. To prepare the crystallized precursors of PEO in toluene, a PEO solution was heated at 70°C for 20 min and incubated at 18°C for 6 hours. The crystallized precursors in the solution were metastable and had a fibrillar morphology that deformed during the spin-coating process. The spin-coating conditions required to obtain a uniformly striped nanopattern were: a spin speed between 2000 and 4000 rpm and a PEO mass fraction in the range 0.2–0.4 wt%. Blocky PEO stripes formed from flat-on lamellar crystals (the chain axis was perpendicular to the substrate) were 10 nm thick, 100 nm wide, and 50 µm long and were arranged in periodic stacks with a period of 200 nm in one direction over a 50 × 50 µm2 area on a silicon wafer. Dense arrangement of the PEO stripes on the silicon wafer during spin-coating produced a grain boundary line in the shape of a distorted hexagonal closed curve (DHCC) on the centimeter length scale. In the DHCC, uniform nanopatterns composed of blocky fibers formed a radial pattern that spread out from a point in the middle of the DHCC to the grain boundary line.

Author and committee

dc:creator, dc:contributor.*
Author
  • 문식원

Identifiers

dc:identifier.*
Identifier
hdl:2014.oak/1808
Mods Identifier Other
OAK-2014-01306

Chain of custody

source
Harvested from
Pohang University of Science and Technology
Base URL
oasis.postech.ac.kr/oai/request
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
related terms
citation

문식원. 용액에서 결정화된 전구체를 이용한 폴리에틸렌 옥사이드 나노 패턴의 박막 제조. 2013. http://postech.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000001557801