Pohang University of Science and Technology
Effect of microstructural parameters on hydrogen delayed fracture of high Mn steels
Abstract
High-Mn twinning-induced plasticity (TWIP) steel is currently attracting much interest in the automotive industry due to its excellent combinations of strength and ductility. Though of its excellent mechanical properties, delayed fracture frequently observed in some high-Mn steels restricts its wide application in the industry. It has well been documented that delayed static fracture is closely related to the hydrogen embrittlement. Hydrogen delayed fracture (HDF) came to the fore as a key issue to be solved for the application of high Mn steels. Although many efforts are being made to improve the HDF resistance of TWIP steels delayed failure mechanism is unclear. For this purpose, hydrogen delayed fracture on high Mn steel was investigated in the context of microstructural parameters, such as ε martensite, dislocation, texture, residual stress and deformation twins.Firstly, effects of ε martensite on HDF behavior of a high Mn steel was investigated. A Fe-15Mn-2Cr-0.6C steel containing various amount of ε martensite (0, 8, 60%) was prepared, and a series of electrochemical hydrogen pre-charging, slow strain rate tests, and thermal desorption spectrometry analyses was conducted to examine the hydrogen degradation behaviors. It was found that ε martensite provided many diffusible hydrogen trapping sites. Consequently, the notch fracture stress of the steel containing ε martensite decreased significantly as the diffusible hydrogen content increased. The activation energy for hydrogen detrapping from its trapping sites was also calculated by means of the thermal desorption spectroscopy analyses, ~22 kJ/mol for the γ/ε interfaces, which is lower than dislocations or γ grain boundaries of ~37 kJ/mol.Secondly, Fe-18Mn-0.6C steels containing various Al content (0 ~3.5% in wt) was studied in the context of hydrogen embrittlement. The roles of residual stress and texture on HDF were discussed. In the deformed state, Al-added TWIP steels exhibited much better delayed fracture resistance as compared to 0 Al steel, owing to the decrease of diffusible hydrogen trapping sites coupled with smaller residual stress and strong <111> and <100> textures.Another effort was made to fabricate high Mn steels in wire rods via cold caliber rolling (CCR), and their microstructure, mechanical properties, and HDF resistance were evaluated. CCR TWIP steels showed a better combination of strength and ductility than conventional bolt steels as a result of CCR inducing all possible <112> twins. The HDF resistance of CCR TWIP steels was excellent due to the inherently low hydrogen diffusivity of the FCC structure and the high density of non-diffusible hydrogen trapping sites (deformation twins).
Author and committee
dc:creator, dc:contributor.*- Author
-
- 전영수
Identifiers
dc:identifier.*- Identifier
- hdl:2014.oak/1831
- Mods Identifier Other
- OAK-2014-01329