Nb2O5 thin film deposited by direct liquid injection-chemical vapor deposition method using Nb(OC2H5)5 precursor

Abstract

The niobium (V) oxide (Nb2O5) is emerging as an advance material for wide range of applications due to its excellent chemical and physical properties. It has attracted much attention as a promising candidate for the future dynamic random access memory and complementary metal oxide semiconductor devices, owing to its high‐κ value of up to 200. The literature studies show that the electrical properties of Nb2O5 are very sensitive to the synthetic routes and deposition conditions. There are several factors that affect the quality of niobium oxide film such as composition (a mixed phase), interface (lattice mismatch, native oxide and transition layer), defect states (oxygen vacancy, interstitial oxygen or metal) and crystal structure (polymorph, texture and grain size) etc. A correlation study between bulk composition and electrical properties has never been reported. In this work, we investigated the effect of growth conditions on film properties. In more details, the influence of reactant’s molar ratios [oxygen: precursor] and deposition temperatures on growth rate, stoichiometry, crystal structure, morphology, dielectric constant and leakage current were studied. The niobium oxide thin films were deposited onto Si (100) substrate by direct liquid injection-chemical vapor deposition method using Nb(OC2H5)5 precursor. Two growth regimes were observed as a function of deposition temperature. The maximum growth rate was observed at a lower oxygen/precursor molar ratio of 150 and deposition temperature of 360 °C. The X-ray photoelectron spectroscopic studies revealed that a mixed phase of niobium oxides (NbO, NbO2 and Nb2O5) in the bulk. The amount of each phase was quite substantial. The higher deposition temperature and oxygen molar ratio results into interface reaction. The films deposited at 340 and 360 °C were amorphous. Therefore, the X-ray diffraction pattern showed the broad peaks. Increasing of oxygen/precursor molar ratios did not help in crystallinity, whereas the grains were formed. Therefore, the grains were weakly crystalline. The crystalline film was obtained at 400 °C and film’s crystallinity was decreased with increase in oxygen molar ratio. The atomic force microscopic image showed a smooth surface for an amorphous film and grains for a weakly crystalline film. The surface roughness of weakly crystalline and crystalline films was very sensitive to the deposition temperatures and reactant’s molar ratios. The capacitance-voltage curve showed a positive shift in flat band voltage was due to excess oxygen and defect state. The capacitance-voltage hysteresis was attributed to the mixed phases of niobium oxide and remained similar as function of deposition condition. The current-voltage curve showed the higher leakage current density for higher surface roughness. It was found that the decrease in surface roughness improved the leakage current. The films dielectric constant was improved by increasing the oxygen ratios. At molar ratio of 150, a high dielectric constant value of 47 at 340 °C was obtained for an amorphous film and corresponding leakage current density was 2.0×10-5 A/cm2 at 1 MV/cm. No break down voltage was observed for any of sample.Further, we investigated the effect of post annealing temperature on composition, crystal structure and electrical property of Nb2O5 in order to obtain a pure crystalline phase. It was monitored that initial growth condition affects the overall film’s properties. The film was deposited at 340 °C under different oxygen ratio R0, R75 and R600 and subsequently post annealed at 500, 600 and 700 °C for 1 hour in Ar gas atmosphere. The films were also deposited at 360 and 400 °C and annealed under same condition for comparison. The film was deposited at 340 °C under R75 and annealed at 500 °C exhibited the mixed states of niobium (Nb2+, Nb4+ and Nb5+)

Author and committee

dc:creator, dc:contributor.*
Author
  • Bharti, Dinesh Chand

Identifiers

dc:identifier.*
Identifier
hdl:2014.oak/2177
Mods Identifier Other
OAK-2014-01675

Chain of custody

source
Harvested from
Pohang University of Science and Technology
Base URL
oasis.postech.ac.kr/oai/request
Last updated
2026-11-26
Source record
OAI-PMH GetRecord
related terms
citation

Bharti, Dinesh Chand. Nb2O5 thin film deposited by direct liquid injection-chemical vapor deposition method using Nb(OC2H5)5 precursor. 2014. http://postech.dcollection.net/jsp/common/DcLoOrgPer.jsp?sItemId=000001676642