Back to search

Technische Universität Dresden

Assessing the autogenous shrinkage cracking propensity of concrete by means of the restrained ring test

Abstract

dc:description.abstract

The autogenous shrinkage due to self-desiccation of high- and ultra-high performance concretes with very low water-cement ratio in case of restraint leads to considerable stresses starting from very early age. The resultant risk of cracking presently cannot be adequately investigated. Parameters that are particularly difficult to capture experimentally are the concrete temperature and the viscoelasticity. The primary objective of this work was to assess as precise as possible the autogenous shrinkage cracking propensity of representative concretes at strong restraint and constant room temperature. Test methods needed to be chosen and enhanced in a way that preferably allowed for the efficient and precise investigation of all relevant factors in the future. Ideally, a method suitable for a complete empirical modeling was provided. First the methodological requirements and the advantages and disadvantages of existing test methods were discussed. Based on this, optimized test methods were proposed. Their suitability was verified using the example of ultra-high strength concrete. The choice of concrete compositions considered the essential measures for reducing shrinkage (internal curing, shrinkage-reducing admixtures, reduction of the fraction of Portland cement in the binder). The autogenous shrinkage was measured with the shrinkage cone method. This new test method was validated by investigations of the repeatability and reproducibility and proved efficient and precise. It allows for measurements under non-isothermal conditions; no established test method exists for that purpose to date. The autogenous shrinkage of the ultra-high strength concretes at the age of 24 h, investigated under quasi-isothermal conditions (20 °C), was between 0,25 mm/m and 0,70 mm/m. It was particularly low when a shrinkage-reducing admixture was added and when superabsorbent polymers were used. The stresses due to restraint were determined with the restrained ring test. A large part of the stresses to be expected according to Hooke’s Law were eliminated by creep and relaxation. The relaxation capacity being very pronounced at very early age was the main reason that no visible cracking occurred, not even with the concretes with high autogenous shrinkage. The development of the autogenous shrinkage cracking propensity was described as ratio of restraint stress and splitting tensile strength. By means of modified ring tests, used to determine the maximum tensile stress, it could be shown that the ratio of stress to strength is an appropriate failure criterion. However, the cracking propensity can be calculated correctly only if the strongly age-dependent ratio of uniaxial to splitting tensile strength is accounted for. Besides, it needs to be considered that at very early age a plastic stress redistribution may occur in restrained ring tests. The reference concrete showed a high cracking propensity of up to 0.68. The fact that shrinkage-reducing measures led to significantly lower values reveals their relevance for the safe application of ultra-high strength concrete. However, the investigations carried out here at 20 °C do not allow for a final assessment of the cracking propensity under typical on-site conditions. To empirically model the autogenous shrinkage cracking propensity as a function of temperature and stress level in the future, an analytical stress solution for non-isothermal restrained ring tests and a new approach for investigating the residual stress and relaxation capacity by means of non-passive restrained ring tests was suggested.

Degree

thesis:*
Level thesis:degree_level
thesis.doctoral
Department thesis:degree_department
Fakultät Bauingenieurwesen
Grantor dc:publisher
Technische Universität Dresden
Year dc:date.issued
2011

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Eppers, Sören
Advisor dc:contributor.advisor
  • Mechtcherine, Viktor

Subjects

dc:subject × 20

Rights

dc:rights.accessrights
Statement dc:rights.accessrights
  • free
  • info:eu-repo/semantics/openAccess
Language dc:language.dcterms_iso639_2
eng

Identifiers

dc:identifier.*
Dc Publisher Identifier
4519974-7
Ddb Identifier Erstkat Id
338924477

Chain of custody

source
Harvested from
QUCOSA
Base URL
www.qucosa.de/oai/
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Eppers, Sören. Assessing the autogenous shrinkage cracking propensity of concrete by means of the restrained ring test. thesis.doctoral thesis, Technische Universität Dresden, 2011. https://nbn-resolving.org/urn:nbn:de:bsz:14-qucosa-65454