Anisotropic hard magnetic nanoparticles and nanoflakes obtained by surfactant-assisted ball milling

Abstract

dc:description.abstract

The research work in this thesis has been devoted to understand the formation mechanism of single-crystalline and textured polycrystalline nanoparticles and nanoflakes of SmCo5 and Nd2Fe14B prepared by surfactant-assisted (SA) ball milling and to study their microstructural and magnetic properties. The nanoparticles and nanoflakes are promising candidates to be used as hard magnetic phase for the fabrication of high-energy-density exchange-coupled nanocomposite magnets. The influence of a range of different surfactants, solvents and milling parameters on the characteristics of ball-milled powder has been systematically investigated. Small fraction (~10 wt.%) of SmCo5 nanoparticles of average diameter 15 nm along with textured polycrystalline nanoflakes of average diameter 1 µm and average thickness of 100 nm were obtained after SA – ball milling of SmCo5 powder. Isolated single-crystalline particles (200-500 nm) and textured polycrystalline flakes (0.2-1.0 µm) of Nd2Fe14B have been prepared in bulk amount (tens of grams), after SA – ball milling of dynamic-hydrogen-disproportionation-desorption-recombination (d-HDDR) processed Nd2Fe14B powder. These single-crystalline Nd2Fe14B particles are promising for their microstructure for the fabrication of exchange-coupled nanocomposite permanent magnets. The SmCo5 and Nd2Fe14B flakes and particles were well aligned in magnetic field: the former showed [001] out-of-plane orientation while the latter showed [001] in-plane orientation. A maximum degree of texture values of 93 % and 88 % have been obtained for the magnetically-oriented SmCo5 flakes and Nd2Fe14B single-crystalline particles, respectively. SA – ball milling resulted in an increase of coercivity of SmCo5 particles from 0.45 T for un-milled powder to a maximum value of 2.3 T after 1 h of milling, further milling resulted in a decrease of the coercivity. The coercivity of SA – ball-milled Nd2Fe14B particles decreased drastically from 1.4 T for un-milled d-HDDR powder to 0.44 T after 0.5 h of milling, isolated single-crystalline particles (200-500 nm size) obtained after 4 h of SA – ball milling showed a coercivity of 0.34 T. The drastic decrease in coercivity of ball-milled Nd2Fe14B particles is attributed to the morphological change because the demagnetization in Nd2Fe14B magnets is governed by nucleation mechanism. A remarkable enhancement in coercivity from 0.26 T to 0.70 T for ethanol-milled sample and from 0.51 T to 0.71 T for oleic-acid-milled samples has been obtained after an optimum heat-treatment at 400 0C. An increase of α-Fe and Nd2O3 phase contents and a sharp change of lattice parameter c of Nd2Fe14B was observed when heat-treating above 400 0C. The change in lattice parameter at higher temperature is thought to be due to partial substitution of carbon atoms present in the surfactant or solvent, for boron atoms.

Degree

thesis:*
Level thesis:degree_level
thesis.doctoral
Department thesis:degree_department
Fakultät Maschinenwesen
Grantor dc:publisher
Technische Universität Dresden
Year dc:date.issued
2016

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Pal, Santosh Kumar
Advisor dc:contributor.advisor
  • Schultz, Ludwig

Subjects

dc:subject × 12

Rights

dc:rights.accessrights
Statement dc:rights.accessrights
  • free
  • info:eu-repo/semantics/openAccess
Language dc:language.dcterms_iso639_2
eng

Identifiers

dc:identifier.*
Dc Publisher Identifier
4519974-7
Ddb Identifier Erstkat Id
856378941

Chain of custody

source
Harvested from
QUCOSA
Base URL
www.qucosa.de/oai/
Last updated
2026-11-27
Source record
OAI-PMH GetRecord
citation

Pal, Santosh Kumar. Anisotropic hard magnetic nanoparticles and nanoflakes obtained by surfactant-assisted ball milling. thesis.doctoral thesis, Technische Universität Dresden, 2016. https://nbn-resolving.org/urn:nbn:de:bsz:14-qucosa-193165