Technische Universität Dresden
Electrical characterization of carbon-hydrogen complexes in silicon and silicon-germanium alloys
Abstract
dc:description.abstractIn this thesis, a comprehensive study of the electrical properties of carbon-hydrogen (CH) complexes in silicon (Si) and silicon-germanium (SiGe) alloys is presented. These complexes form by the reaction of residual carbon impurities with hydrogen that is introduced either by wet chemical etching or a dc hydrogen plasma. The complexes were detected and characterized by the deep level transient spectroscopy (DLTS), Laplace DLTS, and minority carrier transient spectroscopy (MCTS) technique. With this approach, properties like the activation enthalpy for carrier emission, the capture cross section, the charge state, and the thermal stability of the complexes were determined. The composition of the complexes was derived from the analysis of their depth profiles in samples with different impurity concentrations. Using these methods, eight carbon-hydrogen related defect levels (E42, E65, E75, E90, E90', E262, H50, H180) and one hydrogen related level (E150) were detected in Si, SiGe alloys and Ge. Hydrogen plasma treatment at temperatures around 373 K introduces four dominant traps in Si at about Ec-0.06 eV (E42), Ec-0.52 eV (E262), Ev+0.33 eV (H180), and Ev+0.08 eV (H50). E42 and E262 are shown to be two charge states of the same defect. The characteristic field dependence of their emission rate links E42 with the double acceptor level and E262 with the single acceptor level of a CH complex. By comparison of their properties with calculations they are assigned to the anti-bonding configuration of the CH complex (CH_1AB). H180 was previously suggested to be the donor state of the CH_1AB configuration. This hypothesis could not be confirmed. Instead, it is shown that H180 exhibits a barrier for hole capture of about 53 meV, which hinders the reliable determination of its charge state from the field dependence of the emission rate. However, its activation enthalpy is in reasonable agreement with the predicted level position of the acceptor state of the CH_T configuration of CH, where H sits on the tetrahedral interstitial (T) position next to carbon. Therefore, H180 is tentatively assigned to CH_T. H50 is reported for the first time and it appears with concentrations close to the detection limit of the DLTS technique (~1E11 cm^-3). This complicates the determination of its charge state. Nevertheless, theory predicts the acceptor level of the CH_2AB configuration at about Ev+0.07 eV, which is remarkably close to the experimental value of H50. Therefore, H50 is tentatively assigned to the acceptor level of CH_2AB. In contrast, hydrogenation of silicon by wet chemical etching introduces three dominant levels at Ec-0.11 eV (E65), Ec-0.13 eV (E75), and Ec-0.16 eV (E90). Previously, E90 was contradictorily assigned by different authors to the donor and to the acceptor state of the bond-centered configuration of the CH complex (CH_1BC). In this work, this contradiction is resolved. It is shown that two different defect levels (E90 and E90') appear in the DLTS spectra at about 90 K in samples with a low oxygen concentration (< 1E17 cm^-3). The acceptor state of the CH_1BC configuration (E90) can be observed directly after hydrogenation by wet chemical etching or a dc hydrogen plasma treatment at temperatures below 373 K. In contrast, the donor state of a CH_n complex (E90', Ec-0.14 eV), that involves more than one hydrogen atom, is formed by a reverse bias annealing of samples with a net donor concentration of Nd > 1E15 cm^-3. By comparison with theory it is concluded that n > 2. In samples with a high oxygen concentration (> 1E17 cm^-3) E65 and E75 are dominant. Both levels belong to the CH_1BC configuration disturbed by a nearby oxygen atom. The appearance of two levels is the result of two inequivalent positions of the oxygen atom in respect to the CH bond. E42, E90, E262, and H180 are also investigated in diluted SiGe alloys to analyze the influence of alloying on their electrical properties. The presence of Ge atoms in the closest environment of the defects leads to the appearance of additional defect levels close to those observed in pure Si. The relative concentration of these additional defects is in agreement with models of the proposed defect structure of E42, E90, E262, and H180. An increase of the Ge content in SiGe alloys leads to a shift of the defect levels in the band gap of SiGe. An extrapolation of this shift predicts the appearance of E90 and E262 also in pure Ge. A hydrogen related level E150 (Ec-0.31 eV) is indeed observed in hydrogenated n-type Ge. Its concentration is significantly higher after hydrogen plasma treatment than after wet chemical etching. It is shown that E150 contains a single hydrogen atom and involves an unknown impurity, most likely carbon, oxygen, or silicon. E150 represents a reasonable candidate for a CH complex in Ge.
Degree
thesis:*- Level thesis:degree_level
- thesis.doctoral
- Department thesis:degree_department
- Fakultät Mathematik und Naturwissenschaften
- Grantor dc:publisher
- Technische Universität Dresden
- Year dc:date.issued
- 2018
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Stübner, Ronald
- Advisor dc:contributor.advisor
-
- Weber, Jörg
Subjects
dc:subject × 8Rights
dc:rights.accessrights- Statement dc:rights.accessrights
-
- free
- info:eu-repo/semantics/openAccess
- Language dc:language.dcterms_iso639_2
- eng
Identifiers
dc:identifier.*- Dc Publisher Identifier
- 4519974-7
- Ddb Identifier Erstkat Id
- 1018462929