Technische Universität Dresden
Hyperdoping Si with deep-level impurities by ion implantation and sub-second annealing
Abstract
dc:description.abstractIntermediate band (IB) materials have attracted considerable research interest since they can dramatically enhance the near infrared light absorption and lead to applications in the fields of so-called intermediate band solar cells or infrared photodetectors. Hyperdoping Si with deep level impurities is one of the most effective approaches to form an IB inside Si. In this thesis, titanium (Ti) or chalcogen doped Si with concentrations far exceeding the Mott transition limits (~ 5×10^19 cm-3 for Ti) are fabricated by ion implantation followed by pulsed laser annealing (PLA) or flash lamp annealing (FLA). The structural and electrical properties of the implanted layer are investigated by channeling Rutherford backscattering spectrometry (cRBS) and Hall measurements. For Si supersaturated with Ti, it is shown that Ti-implanted Si after liquid phase epitaxy shows cellular breakdown at high doping concentrations during the rapid solidification, preventing Ti incorporation into Si matrix. However, the out-diffusion and the cellular breakdown can be effectively suppressed by solid phase epitaxy during FLA, leading to a much higher Ti incorporation. In addition, the formed microstructure of cellular breakdown also complicates the interpretation of the electrical properties. After FLA, the samples remain insulating even with the highest Ti implantation fluence, whereas the sheet resistance decreases with increasing Ti concentration after PLA. According to the results from conductive atomic force microscopy (C-AFM), the decrease of the sheet resistance after PLA is attributed to the percolation of Ti-rich cellular walls, but not to the insulator-to-metal transition due to Ti-doping. Se-hyperdoped Si samples with different Se concentrations are fabricated by ion implantation followed by FLA. The study of the structural properties of the implanted layer reveals that most Se atoms are located at substitutional lattice sites. Temperature-dependent sheet resistance shows that the insulator-to-metal transition occurs at a Se peak concentration of around 6.3 × 10^20 cm-3, proving the formation of an IB in host semiconductors. The correlation between the structural and electrical properties under different annealing processes is also investigated. The results indicate that the degrees of crystalline lattice recovery of the implanted layers and the Se substitutional fraction depend on pulse duration and energy density of the flash. The sample annealed at short pulse durations (1.3 ms) shows better conductivity than long pulse durations (20 ms). The electrical properties of the hyperdoped layers can be well-correlated to the structural properties resulting from different annealing processes.
Degree
thesis:*- Level thesis:degree_level
- thesis.doctoral
- Department thesis:degree_department
- Fakultät für Mathematik und Naturwissenschaften
- Grantor dc:publisher
- Technische Universität Dresden
- Year dc:date.issued
- 2018
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Liu, Fang
Subjects
dc:subject × 9Rights
dc:rights.accessrights- Statement dc:rights.accessrights
-
- free
- info:eu-repo/semantics/openAccess
- Language dc:language.dcterms_iso639_2
- eng
Identifiers
dc:identifier.*- Dc Publisher Identifier
- 2024114-8
- Ddb Identifier Erstkat Id
- 1663051941