Technische Universität Dresden
Vinyl methyl oxazolidinone as a styrene substitute for unsaturated polyester resins
Abstract
dc:description.abstractSubstituting styrene for unsaturated polyester resin (UPR) formulations is an important subject in industry and research due to styrene's hazardous profile and unpleasant odor. Therefore, this dissertation aimed to find an odorless and low-toxic styrene substitute monomer for UPR formulations providing comparable resin and thermoset properties. Four aspects of styrene substitution were distinguished and investigated. These were direct styrene substitution in conventional UPR formulations, styrene-free formulations providing a high glass transition temperature (Tg ≥ 200 °C) of produced thermosets, exploitation of solubility limits of unsaturated polyesters based on special diols in styrene and in vinyl methyl oxazolidinone as reactive diluent monomers (RDMs), and improvement of storage stability of developed styrene-free UPRs. Despite extensive research, a styrene substitute monomer providing comparable resin and thermoset properties, especially for high-temperature applications, was not found. Therefore, in this dissertation, the search for a suitable styrene substitute monomer began with the high-temperature UPR formulation. It was assumed that styrene substitute monomer for high-temperature applications would serve well for all UPR formulations. The selected high-temperature UP-MPN formulation is based on maleic anhydride, 1,2-propylene glycol, and neopentyl glycol (molar ratio 1.00:0.92:0.21) and corresponds to commercial product used for sheet/bulk molding compound applications. The following monomers were considered as styrene substitutes: 1,4-butanediol dimethacrylate (BDDMA), 2-hydroxyethyl methacrylate (HEMA), dimethyl itaconate (DMI), isobornyl methacrylate (IBOMA), methyl methacrylate (MMA), triethylene glycol dimethacrylate (TEGDMA), and vinyl methyl oxazolidinone (VMOX®). The comparison of the styrene substitute monomers indicated that VMOX® provides a comparable Tg value to styrene (198°C vs. 202°C) and significantly higher Tg value (+30K) than other investigated monomers. However, VMOX®-based resin showed more complex curing behavior in comparison to the styrene-based one. VMOX®-based resin curing reaction is depicted by two exothermic peaks. Very probably, the first curing peak represents the copolymerization of unsaturated polyester and VMOX®. The second curing peak probably represents VMOX® homopolymerization as its temperature maximum (149°C) corresponds with the temperature maximum of the exothermic peak of the VMOX® homopolymerization reaction (142°C). In contrast, the curing reaction of styrene-based resin is depicted by one exothermic curing peak. The VMOX® homopolymerization might be compensated by exchanging VMOX® with DMI as reactive co-diluent monomer. That increases the amount of copolymerization partner for VMOX® and leads to a curing reaction represented by one exothermic peak. Moreover, model experiments regarding the copolymerization of VMOX® with diethyl fumarate (as a model structure for UP) and DMI confirmed the good copolymerization of electron-donating VMOX® double bonds with electron-accepting double bonds of DEF (or UP) as well as DMI. On the other hand, the exchange of VMOX® with DMI decreases the thermoset Tg, due to the lowering of thermoset network stiffness by the flexible DMI structure. A very positive result was low residual monomer content (equal to or lower than 0.5 %) of investigated styrene-based and styrene-free thermosets, which indicated a very effective curing process. In the final step, VMOX® was investigated as styrene substitute monomer for the five UP formulations corresponding to commercial products. The screening indicated similar curing behavior of VMOX-based resins as in the case of VMOX®-and UP-MPN-based resin. In general, the resulting Tg values for styrene- and VMOX®-based thermosets were comparable. Similar effects of VMOX® exchange with DMI were observed for investigated resins and thermosets. The solubility limits of polar isosorbide (ISOS) based UPs in styrene were addressed in the literature. Accordingly, the limited solubility in styrene of UPs based on other special diols like tricyclodecanedimethanol (TCDDM) of polycyclic structure or like 2-ethyl-2-butyl-1,3-propanediol (EBP) and 2-methyl-2-propyl-1,3-propanediol (MPP) with side groups was observed in previous research at FH Münster. Very little research on the solubility of UPs based on special diols in alternative reactive diluent monomers was conducted. After successful styrene substitution in conventional unsaturated polyester formulations, VMOX® was investigated as a RDM for polar ISOS-based UPs as well as EBP-, MPP-, and TCDDM-based UPs. For the solubility investigations, the Hansen Solubility Parameters (HSP) were simulated for UPs as well as for VMOX® and styrene. The solubility tests of various UPs revealed that VMOX® dissolves all investigated amorphous UPs. Therefore, the experimental determination of the VMOX® solubility sphere was not possible. In contrast, not all investigated amorphous UPs were soluble in styrene. Based on the calculated distance parameters (Ra) for each UP and styrene, the radius (R0) of the styrene solubility sphere was experimentally determined. It is 12.71 MPa1/2 for experimentally determined HSPs of RDMs and 12.13 MPa1/2 for QSPR-simulated HSPs of RDMs. In further solubility tests of styrene and VMOX® mixtures, a solubility-promoting effect of VMOX® was discovered. It was found that small amounts of VMOX® (even 1 wt.% for UP-MPP solution in 69 wt.% of styrene) improve the UP solubility in styrene. Decreasing the total RDM content increases the required amount of VMOX® as a solubility promoter. The thermosets produced from resins containing 40 wt.% of each investigated UP and 60 wt.% of VMOX® respectively, achieved glass transition temperatures in the range between 187 °C to 207 °C. Against expectation, the advantage of ISOS rigid structure could not be fully utilized to increase the thermoset Tg, due to decreasing molar mass and decreasing double bond density of ISOS-based UPs. One of the most important aspects of UPR product quality is resin storage stability. In the UPR industry, storage stability of 6 months at room temperature or 100 hours at 80 °C is generally required. A premature gelation of VMOX®-based resins was observed during the development of styrene-free UPRs. The hydroperoxides and peroxyl radicals formed during the polycondensation reaction were assumed to cause the premature gelation of VMOX®-based resins. It was observed that UPs based on fumaric acid and isosorbide are most vulnerable to premature gelation. Therefore, UP-FI was selected for the development of stabilization strategies for VMOX®-based resins. The effectiveness of the stabilization strategy was mainly assessed in storage stability tests at room temperature and in accelerated tests at 80 °C. Additionally, properties such as UP molar mass, UP Tg, resin viscosity, resin curability, and thermoset Tg were investigated. The addition of hindered phenolic primary antioxidants such as Irganox® 1076 and Irganox® 1330, as well as hindered amine light stabilizer Tinuvin® 765 during the resin preparation, turned out to be not ineffective for UP-FI-based resin. However, a slight extension of the resin storage stability time was observed after the addition of 500 to 2000 ppm of Irganox® 1330. As a result, the addition of the stabilizers during unsaturated polyester synthesis was investigated. Eight stabilizer combinations created from hydroquinone (HQ), Irganox® 1330, and phosphoric acid were added respectively at the beginning of the polycondensation process. Subsequently, two UPs were synthesized without Fascat® 4100 (butylstannoic acid) as a catalyst to investigate the catalytic effect of phosphoric acid. From eleven stabilizer and catalyst combinations, the one comprising 400 ppm Fascat® 4100, 500 ppm HQ, 500 ppm Irganox® 1330, and 500 ppm phosphoric acid was selected as the most suitable for VMOX®-based unsaturated polyester resins. It provided the required storage stability time at room temperature as well as at 80 °C, good resin curability, and sufficiently high thermoset Tg. Furthermore, the selected stabilizer combination was applied for the following conventional unsaturated polyesters UP-MPN, UP-MPP1, UP-MPP2, and UP-MTD. Consequently, a significant extension of the storage stability at room temperature and at 80 °C of all VMOX®-based resins was observed. Unfortunately, the selected combination deteriorated the curing reaction, which was expressed by the lower curing enthalpy of each VMOX®-based resin in comparison to the reference. The selected combination did not influence UP-MPN thermoset Tg value; however, it significantly decreased UP-MPP1- and UP-MPP2-based thermosets Tg values. In conclusion, VMOX® is not only able to substitute styrene for conventional unsaturated polyester resin formulations but also creates new possibilities for the development of styrene-free formulations.
Degree
thesis:*- Level thesis:degree_level
- thesis.doctoral
- Grantor dc:publisher
- Technische Universität Dresden
- Year dc:date.issued
- 2025
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Wylezek, Maciej
- Contributors dc:contributor
-
- Voit, Brigitte
- Lorenz, Reinhard
- Bauer, Monika
Subjects
dc:subject × 5Rights
dc:rights- Statement dc:rights
-
- info:eu-repo/semantics/openAccess
- Language dc:language.dcterms_iso639_2
- eng
Identifiers
dc:identifier.*- URN
- urn:nbn:de:bsz:14-qucosa2-992329
- Ddb Identifier Erstkat Id
- 1938286383