Queen's University at Kingston
Durability of Multilayered Textured and Fortified Smooth Polyethylene Geomembranes in Different Geoenvironmental Applications
Abstract
dc:description.abstractThe chemical durability of different modern polyethylene geomembranes (GMBs) is examined to explore their degradation behaviour in different geoenvironmental applications. Jar immersion tests are used to accelerate the degradation of the GMBs in the laboratory at a range of temperatures (25 to 95oC) for 4 to 8 years. The degradation of five textured white electrically conductive and nonconductive multilayered GMBs is examined for municipal solid waste (MSW) and low-level waste (LLW) applications. It is shown that both texturing and adding the conductive layer may affect the service-life of multilayered GMBs. This necessitates investigating the effect of adding functionalized layers on the chemical durability of multilayered GMBs before their use in barrier systems to ensure they can meet the required design life of the application. Considering the three degradation stages of the five multilayered GMBs, the estimated time to nominal failure is at least 20% longer in LLW leachate than in MSW leachate. As such, MSW leachate can be used as a conservative proxy to estimate the service-life of a GMB in contact with LLW leachate. Due to the effect of adding functionalized layers on the durability of multilayered textured GMBs compared to their smooth edge, a double notched approach is introduced to assess the stress crack resistance (SCR) of the textured GMBs. Using this technique on samples taken from the textured and smooth portions at different incubation times, show similar initial and stabilized SCR values but different SCR degradation rates for the different parts of the same GMB roll. Thus, relying solely on SCR values from the smooth edge may underestimate or overestimate the degradation of multilayered textured GMBs. In brine containment applications, the degradation of five fortified smooth GMBs with high initial properties is investigated in different synthetic solutions with different salt concentrations. It is shown that the high initial properties of a GMB may not always be indicative of its long-term performance. Additionally, increasing the salt concentration in the brine solution decreases the rate of GMB degradation due to the higher affinity of the antioxidants to be extracted from the surface of the GMBs in the brine with lower concentrations.
Degree
thesis:*- Department dc:contributor.department
- Civil Engineering
- Grantor
- Queen's University at Kingston
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Zafari, Mohsen
- Advisor dc:contributor.supervisor
-
- Abdelaal, Fady
Subjects
dc:subject × 10Rights
dc:rights- Statement dc:rights
-
- Attribution 4.0 International
- Licence dc:rights.uri
- Language dc:language.iso
- eng
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- https://hdl.handle.net/1974/32531