This thesis aims to develop a material characterization framework for a glass fibre reinforced cured-in-place-pipe (CIPP) liner to evaluate its performance and assess its chemical durability. The test matrix involves two chemical and two mechanical tests, performed in parallel to draw connections between mechanical performance and characteristics of the polymer matrix. Fourier Transform Infrared Spectroscopy (FTIR) is used to assess the functional groups present in the resin, and Differential Scanning Calorimetry (DSC) is used to infer the changes in the chemical microstructure of the material. Three-point bending and uniaxial tension tests are used to characterize the mechanical performance of the liner material. The goal of the first study is to establish the experimental methods and then apply them to assess the effect of curing quality resulting from varied installation conditions. The same CIPP liner was installed in three conditions: one was cured in plant, and two were cured at the GeoEngineering laboratory into a corrugated steel pipe and a buried concrete pipe. Experimental results showed that cure quality varied between installation conditions and had a direct effect on performance, showing a 22% improved buckling capacity and a 49% increase in moment capacity when cured in-plant. Considerations should be made for the external factors (ie. host pipe material, burial depth) during field installations to avoid the repercussions due to lesser curing such as reduced long-term performance. The second study investigates the durability of the same CIPP liner to evaluate long-term behaviour. Accelerated aging conditions involving elevated temperatures and exposure to air and water were used to incubate the material for 1.5 years. The four experiments were used as index tests to analyze degradation, then Time Temperature Superposition techniques were implemented to predict times to nominal degradation. Results showed that water immersion on the external liner side was a critical condition which led to rapid deterioration of the resin and both tensile and flexural ultimate properties. Flexural rigidity trends showed that external buckling capacity remained intact. Service life estimations should be made in consideration of the specific field environment, as this study details the sensitivity of liner durability to exposure conditions.

Degree

thesis:*
Department dc:contributor.department
Civil Engineering
Grantor
Queen's University at Kingston
Year dc:date.issued
2025

Author and committee

dc:creator, dc:contributor.*
Author dc:creator
  • Owens, Abigail Patricia
Advisors dc:contributor.supervisor
  • Abdelaal, Fady
  • Moore, Ian

Subjects

dc:subject × 5

Rights

dc:rights
Statement dc:rights
  • Attribution-NoDerivatives 4.0 International
Language dc:language.iso
eng

Identifiers

dc:identifier.*
Handle dc:identifier.uri
https://hdl.handle.net/1974/35304

Chain of custody

source
Harvested from
Queens University
Base URL
qspace.library.queensu.ca/server/oai/request
Last updated
2026-11-19
Source record
OAI-PMH GetRecord
citation

Owens, Abigail Patricia. The Chemo-Mechanical Characterization of the Long-Term Performance of Glass Fibre Reinforced Cured-in-Place Pipe Liners. Queen's University at Kingston, 2025. https://hdl.handle.net/1974/35304