Queen's University at Kingston
Effects of Mechanical Bonding, Hydration, Thermal Aging, and Exposure Time on Geosynthetic Clay Liners
Abstract
dc:description.abstractThe mechanical and hydraulic performance of conventional and multicomponent geosynthetic clay liners (GCLs) was examined through integrated laboratory and long-term field investigations. This research advances understanding of factors affecting GCL durability in barrier systems, including manufacturing variability, polymer enhancement, coating durability, and long-term environmental degradation. Peel strength testing revealed that polymer coatings provide mechanical bond integrity comparable to thermal treatment. However, coating thickness did not correlate linearly with peel strength, indicating fiber impregnation quality is more critical than coating mass. Accelerated aging of coated GCLs revealed substantial differences in peel strength for different products. The GCL with the thinnest coating showed the fastest antioxidant depletion and the greatest loss of peel strength. A five-parameter model of biphasic antioxidant depletion rates, after applying adjustment factors for realistic one-sided field exposure, suggests that in typical applications at operating temperatures ≤ 25°C with non-aggressive solutions and design lives of 50-100 years, the coatings examined are likely to provide adequate performance, with potential time to OIT depletion extending beyond 300 years in the field. Under simulated cation-exchange conditions, increased reference water content in conventional GCLs further weakened their mechanical bonds. The relationship between hydraulic conductivity and peel strength varied by product type. However, when all GCLs were analyzed together, a positive correlation emerged; higher peel strength was associated with higher hydraulic conductivity. These laboratory findings established a framework for interpreting field-scale GCL performance. The integration of accelerated aging results with hydraulic behavior under chemical and mechanical stresses bridges controlled experiments and long-term field conditions. This framework is further evaluated through data from a 15-year field case study, allowing laboratory-based durability indicators to be examined alongside real-world degradation mechanisms and environmental influences. After 15 years in a cover over arsenic-rich gold mine tailings, it was found that polymer-enhanced products performed similarly to conventional GCLs, suggesting that polymer additives provide benefits only in the early years. All GCLs experienced up to four orders of magnitude increases in hydraulic conductivity due to the combined effects of cation exchange and environmental stressors, including wet-dry and freeze-thaw cycling, root penetration, soil erosion, and mechanical stress from insufficient land-use controls.
Degree
thesis:*- Department dc:contributor.department
- Civil Engineering
- Grantor
- Queen's University at Kingston
- Year dc:date.issued
- 2026
Author and committee
dc:creator, dc:contributor.*- Author dc:creator
-
- Poushimin, Mina
- Advisor dc:contributor.supervisor
-
- Rowe, Kerry
Subjects
dc:subject × 6Rights
dc:rights- Statement dc:rights
-
- Attribution-NoDerivatives 4.0 International
- Licence dc:rights.uri
- Language dc:language.iso
- eng
Identifiers
dc:identifier.*- Handle dc:identifier.uri
- https://hdl.handle.net/1974/36248